Thermal Properties Metric English Comments
Dropping Point 196 °C
385 °F
ConocoPhillips SUPER-STA NLGI No. 2
Description: Conoco Super-STA and Super-STA M Greases are premium-quality, extreme-pressure (EP), multipurpose lithium greases recommended for lubrication of wheel bearings, chassis, ball joints, C...
Dropping Point 196 °C
385 °F
ChevronTexaco Miltex EP NLGI Grade 2
Texaco Miltex EP delivers value through:Good water resistance — Strong resistance to wash out of bearingsGood rust and corrosion protection, even in wet conditionsExtreme pressure protectionProtect..
Dropping Point 196 °C
385 °F
ChevronTexaco PremiumRB
Texaco Premium RB delivers value through:Wide application range — Suitable for high rpm operation, operating temperatures ranging from -34°C to 177°C (-30°F to 350°F) and offers excellent rust ..
Dropping Point 196 °C
385 °F
ConocoPhillips 6+ Brick Grease NLGI No. 6+
Description: Conoco Brick Grease is a hard, amber-colored, smooth-textured, lithium-based grease made in block or brick form. Brick Grease provides a high melting point block grease with good heat r..