Polymer Property : Melting Point = 743 °F
Polymer Property :
Melting Point =
743 °F
Product List
Thermal Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties
Metric
English
Comments
Melting Point
340
-
395
°C
644
-
743
°F
Indium Corp. Indalloy 185 Cadmium Solder Alloy
Information Provided by Indium Corporation