Polymer Property : Melting Point = 644 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 227 - 340 °C
441 - 644 °F
Nihon Superior SN100C4 High Temperature Dipper and Tinning Solder
High temperature dip soldering and tinning of copper wire, polyurethane coated wire and component terminations. For use at up to 400°C.
Melting Point 135 - 340 °C
275 - 644 °F
Average value: 323 °C Grade Count:46
Overview of materials for Polytetrafluoroethylene (PTFE), Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Molded". Each property range of values reported is minimum and maximum v..
Melting Point 320 - 340 °C
608 - 644 °F
Average value: 328 °C Grade Count:22
Overview of materials for Polytetrafluoroethylene (PTFE) Powder
This property data is a summary of similar materials in the MatWeb database for the category "PTFE Powder". Each property range of values reported is minimum and maximum values of appropriate MatWeb..
Melting Point 320 - 340 °C
608 - 644 °F
Melting Range; DTA
Fluorseals PTFE Unfilled
Information provided by TEKU GmbH Fluorkunststoffe, a distributor of Fluorseals materials.
Melting Point 330 - 340 °C
626 - 644 °F
ASTM D3418
Solvay Specialty Polymers Algoflon® L105 Polytetrafluoroethylene (PTFE)
Algoflon® L105 a white PTFE micronized powder produced from dispersion polymerization comprising loose agglomerates of sub-micron sized primary particles. Algoflon® L105 can be de-agglomerate..
Melting Point 330 - 340 °C
626 - 644 °F
ASTM D3418
Solvay Specialty Polymers Algoflon® L106 Polytetrafluoroethylene (PTFE)
Algoflon® L106 a white PTFE micronized powder produced from dispersion polymerization comprising loose agglomerates of sub-micron sized primary particles. Algoflon® L106 can be de-agglomerated..