Melting Point 250 - 258 °C
482 - 496 °F
DSC @ 15°C / min; ASTM D3418
Ovation Polymers RIGITRON 30530 GF Polyester, 30% Glass Reinforced
Polyester – 30 % Glass Fiber Reinforced PET. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. All samples are prepared according to ASTM standards. Va..
Melting Point 250 - 258 °C
482 - 496 °F
DSC @ 15°C / min; ASTM D3418
Ovation Polymers RIGITRON 30545 GF Polyester, 45% Glass Reinforced
Polyester – 45% Glass Fiber Reinforced PET. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. All samples are prepared according to ASTM standards. Var..
Melting Point 252 - 258 °C
486 - 496 °F
DSC
Iran Petrochemical (PCC) TG 621 Polyethylene Terephthalate
Polyethylene Terephthalate fiber grade chips, semi dullApplications: staple fiber, spunbond, meltblown nonwovensInformation provided by Iran Petrochemical Commercial Co.
Melting Point 252 - 258 °C
486 - 496 °F
DSC
Iran Petrochemical (PCC) TG 641 Polyethylene Terephthalate
Polyethylene Terephthalate fiber grade chips, semi dullApplications: staple fiber, textile filament, spunbond, meltblown nonwovensInformation provided by Iran Petrochemical Commercial Co.
Melting Point 252 - 258 °C
486 - 496 °F
DSC
Iran Petrochemical (PCC) TG 641 Super Bright Polyethylene Terephthalate
Polyethylene Terephthalate fiber grade chips, super brightApplications: staple fiber, textile filament, spunbond, meltblown nonwovensInformation provided by Iran Petrochemical Commercial Co.
Melting Point 252 - 258 °C
486 - 496 °F
DSC
Iran Petrochemical (PCC) TG 645 Super Bright Polyethylene Terephthalate
Polyethylene Terephthalate fiber grade chips, super brightInformation provided by Iran Petrochemical Commercial Co.
Melting Point 250 - 258 °C
482 - 496 °F
Isoflon Polyester film
Polyethylene terephthalate film is a flexible film with high mechanical resistance. An excellent insulator, it preserves all its properties in a wide range of temperatures (-70°C to +150°C). ..
Melting Point 252 - 258 °C
486 - 496 °F
DSC
Iran Petrochemical (PCC) TG 645 Polyethylene Terephthalate
Polyethylene Terephthalate fiber grade chipsInformation provided by Iran Petrochemical Commercial Co.
Melting Point 252 - 258 °C
486 - 496 °F
DSC
Iran Petrochemical (PCC) TG 732 Polyethylene Terephthalate
Polyethylene Terephthalate fiber grade chipsInformation provided by Iran Petrochemical Commercial Co.
Copyright © lookpolymers.com All Rights Reserved