Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 210 - 255 °C | 410 - 491 °F | Average value: 225 °C Grade Count:25 |
Overview of materials for Polybutylene Terephthalate (PBT), Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Impact Grade". Each property range of values reported is minimum and m.. |
|||
Melting Point | 215 - 255 °C | 419 - 491 °F | Average value: 240 °C Grade Count:5 |
Overview of materials for PEN-PET This property data is a summary of similar materials in the MatWeb database for the category "PEN-PET". Each property range of values reported is minimum and maximum values of appropriate MatWeb ent.. |
|||
Melting Point | 127 - 255 °C | 260 - 491 °F | Average value: 136 °C Grade Count:101 |
Overview of materials for High Density Polyethylene (HDPE), Ultra High Molecular Weight This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Ultra High Molecular Weight". Each property range of values reported i.. |
|||
Melting Point | 205 - 255 °C | 401 - 491 °F | Average value: 220 °C Grade Count:67 |
Overview of materials for Nylon 6, Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Bead Filled". Each property range of values reported is minimum and maximum values of app.. |
|||
Melting Point | 245 - 255 °C | 473 - 491 °F | |
Indium Corp. Indalloy® 233 Pb-Sb-Sn Solder Alloy Intermediate temp solder. Creep resistant.Information provided by the manufacturer, Indium Corporation. |
|||
Melting Point | 225 - 255 °C | 437 - 491 °F | [10 K/min], ISO 11357 |
Eurotec® Tecodur® PB70 GR15 NL100 KA01 PBT/PET, 15% glass fiber reinforced, heat stabilized, natural, gas injection grade Information provided by Eurotec® |
|||
Melting Point | 225 - 255 °C | 437 - 491 °F | [10 K/min], ISO 11357 |
Eurotec® Tecodur® PB70 GR20 BK002 TD21 PBT/PET, 20% glass fiber reinforced, flame retardant - halogen (RoHS compliant), impact modified, natural Information provided by Eurotec® |
|||
Melting Point | 225 - 255 °C | 437 - 491 °F | [10 K/min], ISO 11357 |
Eurotec® Tecodur® PB70 GR50 BK002 CA01 PBT/PET, 50% glass fiber reinforced, heat & UV stabilized, natural Information provided by Eurotec® |
|||
Melting Point | 225 - 255 °C | 437 - 491 °F | [10 K/min], ISO 11357 |
Eurotec® Tecodur® PB70 GR50 BK009 MX01 PBT/PET, 50% glass fiber reinforced, heat & UV stabilized, improved impact, natural Information provided by Eurotec® |
|||
Melting Point | 245 - 255 °C | 473 - 491 °F | |
Daikin NEOFLON NP-3000 FEP Pellets NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion.Applications: Ultra high speed wire and cable coatings.Information provi.. |
|||
Melting Point | 245 - 255 °C | 473 - 491 °F | Average value: 251 °C Grade Count:25 |
Overview of materials for Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant". Each property range of values re.. |
|||
Melting Point | 246 - 255 °C | 475 - 491 °F | Average value: 252 °C Grade Count:10 |
Overview of materials for Polyethylene Terephthalate (PET), 40% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 40% Glass Reinforced". Specific grades with glass content between 35% .. |
|||
Melting Point | 244 - 255 °C | 471 - 491 °F | Average value: 250 °C Grade Count:15 |
Overview of materials for Polyethylene Terephthalate (PET), 50% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 50% Glass Reinforced". Specific grades with glass content between 45% .. |