Polymer Property : Melting Point = 362 °F
Polymer Property :
Melting Point =
362 °F
Product List
Thermal Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties
Metric
English
Comments
Melting Point
183
-
183
°C
361
-
362
°F
Indium Corp. Indalloy 213 Tin-Lead Solder Alloy
Information Provided by Indium Corporation