Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 129 - 142 °C | 264 - 288 °F | TMA Melt Range |
Huntsman IROGRAN® PS 455-215 TPU-Polyester Polyester-based grades with a broad processing window ideally suited for cast, flat die and flown film lines.Information provided by Alliance Polymers |
|||
Melting Point | 136 - 142 °C | 277 - 288 °F | DSC; ISO 3146 |
Borealis BorPURE™ RB501BF Polypropylene Copolymer BorPure™ RB501BF is a random copolymer. Applications: BorPure™ RB501BF has been developed especially for applications like: food packaging, over wrap film, label film, and shrink film. Additives.. |
|||
Melting Point | 138 - 142 °C | 280 - 288 °F | ISO 3146 |
Borealis Borsoft™ SD233CF High Impact Polypropylene Random Heterophasic Copolymer for Cast Film Borsoft SD233CF is a very soft random heterophasic copolymer, suitable for use on chill roll process. The product combines unique softness with outstanding mechanical properties making it the ideal.. |
|||
Melting Point | 110 - 142 °C | 230 - 288 °F | ISO 3146 |
Borealis Borpeel™ WD255CF PO Compound for Non Sterilizable Peelable Film Applications Borpeel WD255CF is a slip and antiblock agent formulated film resin. It is suitable for the manufacturing of unoriented peelable cast films on chill roll process.Borpeel WD255CF is suitable for vari.. |
|||
Melting Point | 138 - 142 °C | 280 - 288 °F | DSC; ISO 3146 |
Borealis BorPURE™ RD208CF Polypropylene Random Copolymer BorPure™ RD208CF is a random copolymer. This grade is suitable for the manufacturing of unoriented films on chill roll processes. This grade is suitable for the manufacturing of unoriented films o.. |
|||
Melting Point | 138 - 142 °C | 280 - 288 °F | ISO 3146 |
Borealis Borsoft™ SA233CF High Impact Polypropylene Random Heterophasic Copolymer for Blown Film Borsoft SA233CF is a very soft random heterophasic copolymer, suitable for use on conventional blown film lines with air-coolingBorsoft SA233CF is especially suitable for soft packaging, hygienic fi.. |