Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 130 - 133 °C | 266 - 271 °F | |
Polimersan Plastics POLIPOLEN® (Polyethylene) HD-PE 500 PE 500: Polyethylenes with molecular weight higher than 500,000 gr/mol. POLIPOLEN® PE (POLYETHYLENE) is maintained from coke oven gas or from natural gas or from Ethene or Ethane which is produce.. |
|||
Melting Point | 130 - 133 °C | 266 - 271 °F | |
Polimersan Plastics POLIPOLEN® (Polyethylene) UHMW-PE 1000 PE 1000: Polyethylene with very high molecular weight (UHMW - PE 1000; Ultra High Molecular Weight Polyethylene). Polyethylenes with molecular weight higher than 3 million gr/mol. POLIPOLEN® PE (P.. |
|||
Melting Point | 130 - 133 °C | 266 - 271 °F | |
Polimersan Plastics POLIPOLEN® (Polyethylene) HD-PE 500 PE 500: Polyethylenes with molecular weight higher than 500,000 gr/mol. POLIPOLEN® PE (POLYETHYLENE) is maintained from coke oven gas or from natural gas or from Ethene or Ethane which is produce.. |
|||
Melting Point | 129 - 133 °C | 264 - 271 °F | |
Hong Kun Group UV Absorber Chemical Name: 2-(2'-Hydroxy-5'-methylphenyl)benzotriazoleCAS No. 2440-22-4All information provided by Hongkun Group |
|||
Melting Point | 96.0 - 133 °C | 205 - 271 °F | |
Indium Corp. Indalloy 72 Bismuth-Lead-Tin Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 128 - 133 °C | 262 - 271 °F | |
Indium Corp. Indalloy 73 Bismuth-Tin Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 128 - 133 °C | 262 - 271 °F | DIN 53 736 |
Hippe PE 300 Polyethylene Tough, flexible and stiff, depending on the crystalline structure (density). Resinous surface. Excellent dielectric properties, Good resistance against solvents, acids and alkalis. Physiologicall.. |
|||
Melting Point | 130 - 133 °C | 266 - 271 °F | |
Polimersan Plastics POLIPOLEN® (Polyethylene) UHMW-PE 1000 PE 1000: Polyethylene with very high molecular weight (UHMW - PE 1000; Ultra High Molecular Weight Polyethylene). Polyethylenes with molecular weight higher than 3 million gr/mol. POLIPOLEN® PE (P.. |
|||
Melting Point | 126 - 133 °C | 259 - 271 °F | Average value: 131 °C Grade Count:16 |
Overview of materials for High Density Polyethylene (HDPE), Rotational Molding Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Rotational Molding Grade". Each property range of values reported is m.. |