Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 70.0 - 102 °C | 158 - 216 °F | |
Indium Corp. Indalloy 43 Bismuth Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 72.2 - 102 °C | 162 - 216 °F | Average value: 87.9 °C Grade Count:17 |
Overview of materials for Ethylene-Methyl Acrylate Copolymer, Molding Grade This property data is a summary of similar materials in the MatWeb database for the category "Ethylene-Methyl Acrylate Copolymer, Molding Grade". Each property range of values reported is minimum an.. |