Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 335 °C | 635 °F | ASTM D789 |
E-Polymers SEPAZ® C130M 30% Mineral Reinforced LCP Resin Liquid Crystal Polymer Resin: SEPAZ LCP resin has a unique structure and performance unthought of in a traditional plastics. Beside SEPAZ LCP takes the excels in all-around performance and molding .. |
|||
Melting Point | 335 °C | 635 °F | ASTM D789 |
E-Polymers SEPAZ® C130HS 30% Glass Fiber Reinforced High Temperature Stabilized LCP Resin Liquid Crystal Polymer Resin: SEPAZ LCP resin has a unique structure and performance unthought of in a traditional plastics. Beside SEPAZ LCP takes the excels in all-around performance and molding .. |
|||
Melting Point | 335 °C | 635 °F | ASTM D789 |
E-Polymers SEPAZ® C140GM 40% Glass Fiber/Mineral Reinforced LCP Resin Liquid Crystal Polymer Resin: SEPAZ LCP resin has a unique structure and performance unthought of in a traditional plastics. Beside SEPAZ LCP takes the excels in all-around performance and molding .. |
|||
Melting Point | 335 °C | 635 °F | ASTM D789 |
E-Polymers SEPAZ® C140GP 40% Glass Fiber Reinforced LCP Resin Liquid Crystal Polymer Resin: SEPAZ LCP resin has a unique structure and performance unthought of in a traditional plastics. Beside SEPAZ LCP takes the excels in all-around performance and molding .. |