Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 2996 °C | 5425 °F | |
H.C. Starck NRC® 3N5 (UNS R05200) Electron Beam Melted Tantalum Applications: NRC® ETA Tantalum metal products are used where purity and or ductility of the tantalum metal is more important than strength or grain size. Consequently, their primary applicatio.. |
|||
Melting Point | 2996 °C | 5425 °F | |
H.C. Starck NRC® 4N (UNS R05200) Electron Beam Melted Tantalum Applications: NRC® ETA Tantalum metal products are used where purity and or ductility of the tantalum metal is more important than strength or grain size. Consequently, their primary applicatio.. |
|||
Melting Point | 2996 °C | 5425 °F | |
H.C. Starck NRC® 4N5 (UNS R05200) Electron Beam Melted Tantalum Applications: NRC® ETA Tantalum metal products are used where purity and or ductility of the tantalum metal is more important than strength or grain size. Consequently, their primary applicatio.. |
|||
Melting Point | 2996 °C | 5425 °F | |
H.C. Starck NRC® 5N (UNS R05200) Electron Beam Melted Tantalum Applications: NRC® ETA Tantalum metal products are used where purity and or ductility of the tantalum metal is more important than strength or grain size. Consequently, their primary applicatio.. |
|||
Melting Point | 2996 °C | 5425 °F | |
H.C. Starck Ultra 76 Alloy (Ta 2.5%W) Benefits: Significantly improved corrosion resistance in HCl and H2SO4 acids.Minimized hydrogen embrittlement rates compared to standard NRC®76Up to 100 times lower in HCl acidUp to 10 times low.. |