Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 189 °C | 372 °F | ASTM D3418 |
SK Chemicals SKYPEL P128DW Productivity Grade SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plasti.. |
|||
Melting Point | 189 - 192 °C | 372 - 378 °F | |
Shandong Guangyin GYBHVN Polymer Our GYBHVN products are mainly applied in fuel pipes and brake pipes of automobile and hoses of air conditioner.Information provided by Shandong Guangyin |
|||
Melting Point | 189 °C | 372 °F | ISO 11357 |
Suzhou Hipro Polymers Hiprolon® 400 MC HLS G30 Nylon, 30% glass fiber filled Hiprolon® 400 MC HLS G30 is a specialty long chain polyamide compound reinforced with 30% chopped glass fiber for injection molding. It contains some bio-renewable resources Features: high dime.. |
|||
Melting Point | <= 189 °C | <= 372 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil Escorene™ LD 730.09 Blown Ethylene Vinyl Acetate Copolymer Product Description: Escorene Ultra LD 730.09 is a 17.2% vinyl acetate copolymer film resin. LD 730.09 is designed to have superior strength and toughness combined with excellent optics and sealing .. |
|||
Melting Point | <= 189 °C | <= 372 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil Escorene™ LD 730.09 Molding Ethylene Vinyl Acetate Copolymer Product Description: Escorene Ultra LD 730.09 is a high vinyl acetate copolymer with a low melting temperature and excellent strength properties and toughness.Availability: Latin America, North Amer.. |
|||
Melting Point | 189 °C | 372 °F | ISO 11357 |
Arkema Group Rilsan® PA 11 G BMNO MED Nylon 11 Rilsan® PA 11 G BMNO MED is a polyamide produced from a renewable source. This grade offers the highest quality and it is specially designed to meet the stringent requirements of the medical applic.. |
|||
Melting Point | 189 °C | 372 °F | ASTM D3418 |
ALM PA 850-Nat Nylon 11 SLS Prototyping Polymer Unfilled PA 11 formulated for easy processing. Can be run as a drop-in replacement for other commercially available PA 11 laser sintering powders. Parts produced from PA 850 exhibit outstanding mech.. |
|||
Melting Point | 189 °C | 372 °F | |
BASF Ultramid® C40 LN 07 0.04 mm Blown Film Cold Air Information provided by BASF |
|||
Melting Point | 189 °C | 372 °F | ASTM D3418 |
ALM FR 106 Nylon 11 SLS Prototyping Polymer This flame retardant rapid prototyping material has additives in the raw material that allows it to pass aeronautic standard FAR25.853 smoke, flame, and toxicity tests. This material is ideal for Ae.. |
|||
Melting Point | 189 °C | 372 °F | ASTM D2117 |
Samyang Triel® 5300 Thermoplastic Polyether Ester Elastomer TRIEL® resins offer superior mechanical properties, elasticities, heat and chemical resistance, which allow it to be widely used for electric/electronic equipments, automotive parts and outdoor rec.. |
|||
Melting Point | 189 - 192 °C | 372 - 378 °F | |
Shandong Guangyin GYBHVNP Polymer Our GYBHVNP products are mainly applied in fuel pipes and brake pipes of automobile and hoses of air conditioner.Information provided by Shandong Guangyin |