Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 2000 °C | 3630 °F | |
Johnson Matthey Yara 58-Y1 N2O Abatement Catalyst Odorless solid pellets, 9 x 9 mm. During the manufacture of Nitric Acid, significant quantities of pollutants are released into the atmosphere. One of the principal pollutants is the greenhouse gas.. |
|||
Melting Point | >= 2000 °C | >= 3630 °F | |
Zircar Refractory Composites RS-3000 ALUMINA FELT ZRCI Alumina Felt Type RS-3000 is 97% high purity alumina fiber, ceramic felt with less than 1% shot. Type RS-3000 is a strong, flexible material with fibers held together with an organic binder. It.. |
|||
Melting Point | 2000 °C | 3630 °F | |
3M Nextel™ 610 Composite Ceramic Fiber Chemical composition above is wt%. Filament diameter is 10-12 µm.3M Nextel Ceramic Fibers 610, 650, and 720 are composite grade fibers. They have a refined crystal structure based on alpha-Al2O3 .. |
|||
Melting Point | 2000 °C | 3630 °F | |
3M Nextel™ DF-11 Woven Fabric 610 Information provided by 3M |
|||
Melting Point | 2000 °C | 3630 °F | |
3M Nextel™ DF-19 Woven Fabric 610 Information provided by 3M |