Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 166 °C | 331 °F | ASTM D1525 |
Kolon KOCETAL® K300BK Black Colored Grade Acetal Resin Colored, general purpose injection molding grade. Applications: General injection molding products.Information provided by API-Kolon. |
|||
Melting Point | 166 °C | 331 °F | DSC; ISO 3146 |
Borealis Borpact™ BC918CF Polypropylene Copolymer Borpact™ BC918CF is a high crystalline heterophasic copolymer film resin, based on special Borstar® nucleating technology. Optical properties will not be deteriorated as with conventional homo or .. |
|||
Melting Point | 166 °C | 331 °F | 10°C/min; ISO 11357-1/-3 |
Barlog Plastics KEBAFORM C 50.0 POM Copolymer unreinforced POMInformation provided by BARLOG plastics GmbH. |
|||
Melting Point | 166 °C | 331 °F | 10°C/min; ISO 11357-1/-3 |
Barlog Plastics KEBAFORM C 901 TF POM Copolymer unreinforced, improved wear and friction POMInformation provided by BARLOG plastics GmbH. |
|||
Melting Point | 166 °C | 331 °F | 10°C/min; ISO 11357-1/-3 |
Barlog Plastics KEBAFORM C 902 FA POM Copolymer unreinforced, reduced formaldehyde emission, UV-stabilized POMInformation provided by BARLOG plastics GmbH. |
|||
Melting Point | 166 °C | 331 °F | 10°C/min; ISO 11357-1/-3 |
Barlog Plastics KEBAFORM C 902 TF POM Copolymer unreinforced, improved wear and friction POMInformation provided by BARLOG plastics GmbH. |
|||
Melting Point | 166 °C | 331 °F | 10°C/min; ISO 11357-1/-3 |
Barlog Plastics KEBAFORM C 903 LF POM Copolymer unreinforced, improved wear and friction POMInformation provided by BARLOG plastics GmbH. |
|||
Melting Point | 166 °C | 331 °F | DIN 53765 |
BASF Ultraform H 4320 Q600 POM Ultraform H4320 Q600 is an extrusion POM high molecular weight grade. This grade enables high extrusion rates with thick-walled product. It also exhibits high thermal stability and a low tendency .. |
|||
Melting Point | 166 °C | 331 °F | ISO 3146 |
Azdel Plus R301B01N 30% Continuous Random Fiber Mat / PP Resin Matrix AZDEL® R301B01N is a random oriented needled continuous glass fiber mat material. This polypropylene composite material features high properties and a basic homogeneous fiber distribution. This m.. |
|||
Melting Point | 166 °C | 331 °F | 10K/min; ISO 3146 |
CENTROPLAST CENTRODAL GL Polyoxymethylene + PE-UHMW CENTRODAL GL has good dry running and emergency running properties. During the modification of POM + PE, a PE-UHMW is incorporated to the basic polyoxymethylene polymer. It leads to an improvement.. |