Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 1400 - 1430 °C | 2550 - 2610 °F | |
Kennametal Stellite Denertia™ C14 Cobalt Chromium Dental Alloy Denertia™ C14 is a cobalt chromium base-metal casting alloy for the manufacture of removable partial dentures and bridgework. It conforms to the following International Standards: EN 1641 §.. |
|||
Melting Point | 1400 - 1440 °C | 2550 - 2620 °F | |
Special Metals DURANICKEL® 301 (UNS N03301) Annealed and Aged Wire Tensile strength (ultimate) and elongation values reported here are typical for Annealed and Aged Wire specifically. Other property values are typical of aged DURANICKEL® alloy 301 or the alloy i.. |
|||
Melting Point | 1400 - 1440 °C | 2550 - 2620 °F | |
Special Metals DURANICKEL® 301 (UNS N03301) Annealed Strip Tensile strength (ultimate and yield), hardness, and elongation values reported here are typical for Annealed Strip specifically. Other property values are typical of annealed DURANICKEL® alloy 3.. |
|||
Melting Point | 1400 - 1440 °C | 2550 - 2620 °F | |
Special Metals DURANICKEL® 301 (UNS N03301) Cold-Drawn Rod and Bar Tensile strength (ultimate and yield), hardness, and elongation values reported here are typical for Cold-Drawn Rod and Bar specifically. Other property values are typical of annealed DURANICKEL®.. |
|||
Melting Point | 1400 - 1440 °C | 2550 - 2620 °F | |
Special Metals DURANICKEL® 301 (UNS N03301) Hot-Finished Rod and Bar Tensile strength (ultimate and yield), hardness, and elongation values reported here are typical for Hot-Finished Rod and Bar specifically. Other property values are typical of annealed DURANICKELÂ.. |
|||
Melting Point | 1400 - 1440 °C | 2550 - 2620 °F | |
Special Metals DURANICKEL® 301 (UNS N03301) Spring Wire Tensile strength (ultimate) and elongation values reported here are typical for Spring Wire specifically. Other property values are typical of annealed DURANICKEL® alloy 301 or the alloy in gener.. |
|||
Melting Point | 1400 °C | 2550 °F | |
Goodfellow Cobalt 90/Aluminum 10 Alloy Information provided by Goodfellow. |
|||
Melting Point | 1400 - 1450 °C | 2550 - 2640 °F | |
Goodfellow Iron 50/Nickel 50 Alloy Information provided by Goodfellow. |
|||
Melting Point | 1400 - 1450 °C | 2550 - 2640 °F | |
Goodfellow Iron 55/Nickel 45 Alloy Low Nickel magnetic alloy. Most applications are based on the requirements of moderately high saturation and permeabilities greater than silicon irons. Uses include the manufacture of sensitive rela.. |
|||
Melting Point | 1400 - 1420 °C | 2550 - 2590 °F | |
Crucible Steel 303 Plus Chromium-Nickel Steel Crucible 303 Plus is a non-hardenable austenitic chromium-nickel steel to which elements have been added to improve machinability and non-galling characteristics. Better machinability than that of.. |
|||
Melting Point | 1399 - 1454 °C | 2550 - 2649 °F | |
AK Steel 201LN Austenitic Stainless steel AK Steel 210 was developed originally to conserve nickel. It provides properties similar to Type 301 and can be used in most applications for Type 301. This alloy is non-magnetic in the annealed c.. |
|||
Melting Point | 1399 - 1421 °C | 2550 - 2590 °F | |
AK Steel 301 Austenitic Stainless steel AK Steel 301 provides high strength and good ductility when cold worked. It is a modification of AK Steel 302 to increase the cold work-hardening range, to permit higher tensile strengths to be ach.. |
|||
Melting Point | 1399 - 1454 °C | 2550 - 2649 °F | |
AK Steel 305 Austenitic Stainless steel AK Steel 305 can be spun and deep drawn more easily due to an increased nickel content that decreases work hardening. It is non-magnetic and cannot be hardened by heat treatment. Typical uses incl.. |
|||
Melting Point | 1399 - 1510 °C | 2550 - 2750 °F | |
ATI Allegheny Ludlum Martensitic Stainless Steel Type 440A, Hardened + 288°C Temper Allegheny Ludlum Type 440A is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainle.. |
|||
Melting Point | 1399 - 1421 °C | 2550 - 2590 °F | |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 304, 50% Cold Rolled (UNS S30400) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Melting Point | 1399 - 1421 °C | 2550 - 2590 °F | |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 304L, 0% Cold Rolled (UNS S30403) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Melting Point | 1399 - 1421 °C | 2550 - 2590 °F | |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 304L, 10% Cold Rolled (UNS S30403) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Melting Point | 1399 - 1421 °C | 2550 - 2590 °F | |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 304L, 60% Cold Rolled (UNS S30403) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Melting Point | 1399 - 1421 °C | 2550 - 2590 °F | |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 305, 40% Cold Rolled (UNS S30500) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Melting Point | 1399 - 1421 °C | 2550 - 2590 °F | |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 305, Annealed (UNS S30500) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Melting Point | 1400 - 1455 °C | 2550 - 2651 °F | |
ATI Allegheny Ludlum Stainless Steel Type 201, 40% Cold Work (UNS S20100) Allegheny Ludlum Type 201 and 201L have the greatest tonnage of the Cr-Ni-Mn steels (200 series). Type 201 provides advantages over the 18-8 grades in certain applications. Lower cost manganese an.. |
|||
Melting Point | 1400 - 1455 °C | 2550 - 2651 °F | |
ATI Allegheny Ludlum Stainless Steel Type 201, 50% Cold Work (UNS S20100) Allegheny Ludlum Type 201 and 201L have the greatest tonnage of the Cr-Ni-Mn steels (200 series). Type 201 provides advantages over the 18-8 grades in certain applications. Lower cost manganese an.. |
|||
Melting Point | 1400 - 1455 °C | 2550 - 2651 °F | |
ATI Allegheny Ludlum Stainless Steel Type 201L, 10% Cold Work (UNS S20103) Allegheny Ludlum Types 201 and 201L have the greatest tonnage of the Cr-Ni-Mn steels (200 series). Type 201L provides advantages over the 18-8 grades in certain applications. Lower cost manganese .. |
|||
Melting Point | 1399 - 1421 °C | 2550 - 2590 °F | |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 304, 30% Cold Rolled (UNS S30400) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Melting Point | 1399 - 1421 °C | 2550 - 2590 °F | |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 304, 40% Cold Rolled (UNS S30400) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Melting Point | 1400 - 1455 °C | 2550 - 2651 °F | |
ATI Allegheny Ludlum Stainless Steel Type 201, 20% Cold Work (UNS S20100) Allegheny Ludlum Type 201 and 201L have the greatest tonnage of the Cr-Ni-Mn steels (200 series). Type 201 provides advantages over the 18-8 grades in certain applications. Lower cost manganese an.. |
|||
Melting Point | 1399 - 1421 °C | 2550 - 2590 °F | |
ATI Allegheny Ludlum Stainless Steel Type 301, annealed (UNS S30100) Allegheny Ludlum Type 301 is a high strength grade of steel available in six conditions or tempers, its resistance to atmosphere corrosion and its bright, attractive surface make it an excellent cho.. |
|||
Melting Point | 1400 °C | 2550 °F | |
Resistalloy International Resistalloy 8020 Nickel Chromium Electrical Resistance Alloy Used mainly for electrical elements in both industrial and domestic applications. Industrial applications vary from small laboratory kilns to heavy-duty heat-treatment furnaces under all types of at.. |
|||
Melting Point | 1400 - 1455 °C | 2550 - 2651 °F | |
ATI Allegheny Ludlum Stainless Steel Type 201L, 40% Cold Work (UNS S20103) Allegheny Ludlum Types 201 and 201L have the greatest tonnage of the Cr-Ni-Mn steels (200 series). Type 201L provides advantages over the 18-8 grades in certain applications. Lower cost manganese .. |