Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 1390 - 1440 °C | 2530 - 2620 °F | |
Kennametal Stellite Denertia™ C4 Cobalt Chromium Dental Alloy Denertia™ C4 is a cobalt chromium base-metal casting alloy for the manufacture of removable partial dentures and bridgework.It conforms to the following International Standards: EN 1641 §4... |
|||
Melting Point | 1390 - 1430 °C | 2530 - 2610 °F | |
Special Metals INCONEL® Alloy 751 A nickel-chromium alloy similar to INCONEL ALLOY X-750 but with increased aluminum content for greater precipitation hardening. INCONEL alloy 751 was designed for use as exhaust valves in internal-.. |
|||
Melting Point | 1390 - 1430 °C | 2530 - 2610 °F | |
Special Metals INCONEL® Alloy X-750 A nickel-chromium alloy similar to INCONEL alloy 600 but made precipitation hardenable by additions of aluminum and titanium. The alloy has good resistance to corrosion and oxidation along with hig.. |
|||
Melting Point | 1390 °C | 2530 °F | |
Goodfellow Zirconium 56.5/Vanadium 43.5 Alloy Information provided by Goodfellow. |
|||
Melting Point | 1388 °C | 2530 °F | |
ATI Allegheny Ludlum AL 22™ Nickel-Base Alloy, UNS N06022 AL 22 alloy is a Ni-Cr-Mo alloy that provides outstanding resistance to pitting, crevice corrosion, intergranular attack, and stress corrosion cracking. The combination of Cr, Ni, Mo, and W provide.. |
|||
Melting Point | 1390 - 1440 °C | 2530 - 2620 °F | |
ATI Allegheny Ludlum Type 317 Stainless Steel, UNS S31700 This is a molybdenum-bearing austenitic stainless steels which is more resistant to general corrosion and pitting/crevice corrosion than the conventional chromium-nickel austenitic stainless steels .. |
|||
Melting Point | 1390 - 1440 °C | 2530 - 2620 °F | |
ATI Allegheny Ludlum Type 316 Stainless Steel, UNS S31600 This is a molybdenum-bearing austenitic stainless steels which is more resistant to general corrosion and pitting/crevice corrosion than the conventional chromium-nickel austenitic stainless steels .. |
|||
Melting Point | 1390 - 1440 °C | 2530 - 2620 °F | |
ATI Allegheny Ludlum Type 316L Stainless Steel, UNS S31603 This is a molybdenum-bearing austenitic stainless steels which is more resistant to general corrosion and pitting/crevice corrosion than the conventional chromium-nickel austenitic stainless steels .. |
|||
Melting Point | 1390 °C | 2530 °F | |
Resistalloy International Resistalloy 3718 Nickel Chromium Electrical Resistance Alloy Used mainly for electrical elements in both industrial and domestic applications. Industrial applications vary from small laboratory kilns to heavy-duty heat-treatment furnaces under all types of at.. |
|||
Melting Point | 1390 °C | 2530 °F | |
Resistalloy International Resistalloy 6015 Nickel Chromium Electrical Resistance Alloy Used mainly for electrical elements in both industrial and domestic applications. Industrial applications vary from small laboratory kilns to heavy-duty heat-treatment furnaces under all types of at.. |