Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 1150 - 1260 °C | 2100 - 2300 °F | |
IBC Advanced Alloys 41C Beryllium Nickel Casting Alloy Beryllium nickel casting alloys are characterized by their steel-like high strength, toughness, and hardness properties. However, unlike the steel alloys, the beryllium nickel alloy system offers th.. |
|||
Melting Point | 1150 - 1260 °C | 2100 - 2300 °F | |
IBC Advanced Alloys 42C Beryllium Nickel Casting Alloy Beryllium nickel casting alloys are characterized by their steel-like high strength, toughness, and hardness properties. However, unlike the steel alloys, the beryllium nickel alloy system offers th.. |
|||
Melting Point | 1150 - 1260 °C | 2100 - 2300 °F | |
IBC Advanced Alloys 43C Beryllium Nickel Casting Alloy Beryllium nickel casting alloys are characterized by their steel-like high strength, toughness, and hardness properties. However, unlike the steel alloys, the beryllium nickel alloy system offers th.. |
|||
Melting Point | 1150 - 1260 °C | 2100 - 2300 °F | |
IBC Advanced Alloys 44C Beryllium Nickel Casting Alloy Beryllium nickel casting alloys are characterized by their steel-like high strength, toughness, and hardness properties. However, unlike the steel alloys, the beryllium nickel alloy system offers th.. |
|||
Melting Point | 1150 - 1260 °C | 2100 - 2300 °F | |
IBC Advanced Alloys 46C Beryllium Nickel Casting Alloy Beryllium nickel casting alloys are characterized by their steel-like high strength, toughness, and hardness properties. However, unlike the steel alloys, the beryllium nickel alloy system offers th.. |
|||
Melting Point | 1150 °C | 2100 °F | |
IBC Advanced Alloys 6% BeNi Beryllium Nickel Master Alloy Beryllium nickel “Master Alloys†are formulated to introduce relatively small percentage “alloying†additions to base metal furnace melts. Producers of aluminum, magnesium, and n.. |
|||
Melting Point | 1150 - 1315 °C | 2100 - 2399 °F | |
Materion Beryllium Nickel M220C Information supplied by Brush Wellman Engineered Materials.Brush M220C is characterized by high levels of strength, hardness, and thermal conductivity combined with excellent resistance to wear, cor.. |
|||
Melting Point | 1150 - 1220 °C | 2100 - 2230 °F | |
Wieland 1751 Wilaform Palladium Approach-steady palladium alloy for nearly all purposes in decoration manufacturingApplications: casting, chains, laminar decoration, pipes, tubingDental |
|||
Melting Point | 1150 °C | 2100 °F | |
Goodfellow Zirconium 70/Nickel 30 Alloy Information provided by Goodfellow. |
|||
Melting Point | 1150 - 1170 °C | 2100 - 2140 °F | |
CLAL-MSX ARCAP Anticorrosion AP1 0 Annealed, Drawn Copper Alloy Description: The AP1D grade has been developed especially for being machined by lathe. Its machineability is one of the best of all of the corrosion resistant alloys. The very good machineability of.. |
|||
Melting Point | 1150 - 1170 °C | 2100 - 2140 °F | |
CLAL-MSX ARCAP Anticorrosion AP1 0 Annealed, Rolled Copper Alloy Description: The AP1D grade has been developed especially for being machined by lathe. The very good machineability of the AP1D grade may be summerised by: cutting speed up to 150 m/minute (accordin.. |
|||
Melting Point | 1150 - 1170 °C | 2100 - 2140 °F | |
CLAL-MSX ARCAP Anticorrosion AP1 H12 1/2 hard, Drawn Copper Alloy Description: The AP1D grade has been developed especially for being machined by lathe. The very good machineability of the AP1D grade may be summerised by: cutting speed up to 150 m/minute (accordin.. |
|||
Melting Point | 1150 - 1170 °C | 2100 - 2140 °F | |
CLAL-MSX ARCAP Anticorrosion AP1 H12 1/2 hard, Rolled Copper Alloy Description: The AP1D grade has been developed especially for being machined by lathe. The very good machineability of the AP1D grade may be summerised by: cutting speed up to 150 m/minute (accordin.. |
|||
Melting Point | 1150 - 1170 °C | 2100 - 2140 °F | |
CLAL-MSX ARCAP Anticorrosion AP1 H13 3/4 hard, Drawn Copper Alloy Description: The AP1D grade has been developed especially for being machined by lathe. The very good machineability of the AP1D grade may be summerised by: cutting speed up to 150 m/minute (accordin.. |
|||
Melting Point | 1150 - 1170 °C | 2100 - 2140 °F | |
CLAL-MSX ARCAP Anticorrosion AP1 H14 4/4 hard, Rolled Copper Alloy Description: The AP1D grade has been developed especially for being machined by lathe. The very good machineability of the AP1D grade may be summerised by: cutting speed up to 150 m/minute (accordin.. |
|||
Melting Point | 1150 - 1170 °C | 2100 - 2140 °F | |
CLAL-MSX ARCAP Anticorrosion AP1C 0 Annealed, Drawn Copper Alloy Description: The AP1C grade (used in rods for parts that are to be deformed by torsion, bending, riveting, swaging... and for welding) and the AP1 grade (sheet, strip, wire, tubes) is machineable un.. |
|||
Melting Point | 1150 - 1170 °C | 2100 - 2140 °F | |
CLAL-MSX ARCAP Anticorrosion AP1C H12 1/2 hard, Rolled Copper Alloy Description: The AP1C grade (used in rods for parts that are to be deformed by torsion, bending, riveting, swaging... and for welding) and the AP1 grade (sheet, strip, wire, tubes) is machineable un.. |
|||
Melting Point | 1150 - 1170 °C | 2100 - 2140 °F | |
CLAL-MSX ARCAP Anticorrosion AP1C H13 3/4 hard, Drawn Copper Alloy Description: The AP1C grade (used in rods for parts that are to be deformed by torsion, bending, riveting, swaging... and for welding) and the AP1 grade (sheet, strip, wire, tubes) is machineable un.. |
|||
Melting Point | 1150 - 1170 °C | 2100 - 2140 °F | |
CLAL-MSX ARCAP Anticorrosion AP1C H13 3/4 hard, Rolled Copper Alloy Description: The AP1C grade (used in rods for parts that are to be deformed by torsion, bending, riveting, swaging... and for welding) and the AP1 grade (sheet, strip, wire, tubes) is machineable un.. |
|||
Melting Point | 1150 - 1170 °C | 2100 - 2140 °F | |
CLAL-MSX ARCAP Anticorrosion AP1C H14 4/4 hard, Drawn Copper Alloy Description: The AP1C grade (used in rods for parts that are to be deformed by torsion, bending, riveting, swaging... and for welding) and the AP1 grade (sheet, strip, wire, tubes) is machineable un.. |
|||
Melting Point | 1150 - 1170 °C | 2100 - 2140 °F | |
CLAL-MSX ARCAP Anticorrosion AP1 H11 1/4 hard, Drawn Copper Alloy Description: The AP1D grade has been developed especially for being machined by lathe. The very good machineability of the AP1D grade may be summerised by: cutting speed up to 150 m/minute (accordin.. |
|||
Melting Point | 1150 - 1170 °C | 2100 - 2140 °F | |
CLAL-MSX ARCAP Anticorrosion AP1 H11 1/4 hard, Rolled Copper Alloy Description: The AP1D grade has been developed especially for being machined by lathe. The very good machineability of the AP1D grade may be summerised by: cutting speed up to 150 m/minute (accordin.. |
|||
Melting Point | 1150 - 1170 °C | 2100 - 2140 °F | |
CLAL-MSX ARCAP Anticorrosion AP1 H15 Spring, Drawn Copper Alloy Description: The AP1D grade has been developed especially for being machined by lathe. The very good machineability of the AP1D grade may be summerised by: cutting speed up to 150 m/minute (accordin.. |
|||
Melting Point | 1150 - 1170 °C | 2100 - 2140 °F | |
CLAL-MSX ARCAP Anticorrosion AP1C H11 1/4 hard, Drawn Copper Alloy Description: The AP1C grade (used in rods for parts that are to be deformed by torsion, bending, riveting, swaging... and for welding) and the AP1 grade (sheet, strip, wire, tubes) is machineable un.. |
|||
Melting Point | 1150 - 1170 °C | 2100 - 2140 °F | |
CLAL-MSX ARCAP Anticorrosion AP1C H11 1/4 hard, Rolled Copper Alloy Description: The AP1C grade (used in rods for parts that are to be deformed by torsion, bending, riveting, swaging... and for welding) and the AP1 grade (sheet, strip, wire, tubes) is machineable un.. |
|||
Melting Point | 1150 - 1170 °C | 2100 - 2140 °F | |
CLAL-MSX ARCAP Anticorrosion AP1C H14 4/4 hard, Rolled Copper Alloy Description: The AP1C grade (used in rods for parts that are to be deformed by torsion, bending, riveting, swaging... and for welding) and the AP1 grade (sheet, strip, wire, tubes) is machineable un.. |
|||
Melting Point | 1150 - 1170 °C | 2100 - 2140 °F | |
CLAL-MSX ARCAP Anticorrosion AP1C H15 Spring, Drawn Copper Alloy Description: The AP1C grade (used in rods for parts that are to be deformed by torsion, bending, riveting, swaging... and for welding) and the AP1 grade (sheet, strip, wire, tubes) is machineable un.. |
|||
Melting Point | 1150 - 1170 °C | 2100 - 2140 °F | |
CLAL-MSX ARCAP Anticorrosion AP1D H14 4/4 hard, Drawn Copper Alloy, Wire and rod, 2.5< diameter< 5 High Corrosion Resistance: ARCAP alloys are very corrosion resistant to the majority of chemical and physical environments. CLAL can provide data for the corrosion resistance of ARCAP alloys. In par.. |
|||
Melting Point | 1150 - 1170 °C | 2100 - 2140 °F | |
CLAL-MSX ARCAP Anticorrosion AP1D H14 4/4 hard, Drawn Copper Alloy, Wire and rod, diameter High Corrosion Resistance: ARCAP alloys are very corrosion resistant to the majority of chemical and physical environments. CLAL can provide data for the corrosion resistance of ARCAP alloys. In par.. |