Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 851 °C | 1560 °F | |
Solvay Chemicals Soda Solvay® Dense Soda Ash (European Grade) Soda Ash Dense is the grade preferred for glass manufacture because its granular properties make it dust-free and reduce the risks of segregation during transport and handling.Applications: Glass in.. |
|||
Melting Point | 851 °C | 1560 °F | |
Solvay Chemicals Soda Solvay® Light Soda Ash (European Grade) Soda Ash Dense is the grade preferred for glass manufacture because its granular properties make it dust-free and reduce the risks of segregation during transport and handling.Applications: Glass in.. |
|||
Melting Point | 851 °C | 1560 °F | |
Solvay Chemicals Soda Solvay® Dense Soda Ash Soda Ash Dense is the grade preferred for glass manufacture because its granular properties make it dust-free and reduce the risks of segregation during transport and handling.Applications: Glass in.. |
|||
Melting Point | 850 - 880 °C | 1560 - 1620 °F | |
Wieland 1401 Wilaform Gold Hard standard yellow gold alloy. Easily splintered and polished thus very well suited for crafts and industrial decoration manufacturing.Applications: casting, chains, laminar decoration, pipes, tu.. |
|||
Melting Point | 850 - 900 °C | 1560 - 1650 °F | |
Williams Advanced Alloys Wambraze™ WB900B Solder High-purity vacuum cast materials are manufactured by Williams in a variety of solder alloys, including gold brazing alloys for electronic packaging and high temperature joining vacuum electronic de.. |