Thermal Properties Metric English Comments
Melting Point -75.0 °C
-103 °F
Freezing Point
LG Chemical Ethyl Acrylate
Features: Low Color - Refining process are improved for produce the low color. Color is the main quality factor that influence the property of the final products. Low Acidity - Through the multistag..
Melting Point -75.0 °C
-103 °F
Freezing Point
LG Chemical Methyl Acrylate
Features: Low Color - Refining process are improved for produce the low color. Color is the main quality factor that influence the property of the final products. Low Acidity - Through the multistag..
Melting Point <= -75.0 °C
<= -103 °F
BASF 2-Ethylhexanoyl Chloride
Formula: C8H15ClOCAS: 760-67-8Description: 2-Ethylhexanoyl chloride is a colorless to yellowish liquid with a pungent odor. It is miscible with all common organic solvents. It hydrolyses in the pres..
Melting Point -75.0 °C
-103 °F
Freezing Point
BASF Methyl Acrylate
Formula: C4H6O2CAS: 96-33-3Description: Acrylic ester for manufacturing polymers and for use as a feedstock for syntheses. Applications: Methyl acrylate forms homopolymers and copolymers. Copolymer..
Melting Point -75.0 - 143 °C
-103 - 289 °F
Average value: 74.6 °C Grade Count:34
Overview of materials for Ethylene Butyl Acrylate
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Butyl Acrylate". Each property range of values reported is minimum and maximum values of approp..