Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 632 - 654 °C | 1170 - 1210 °F | AA 5005 |
Aleris 55HX® Aluminum (5005-H14) Used in interior and exterior architectural applications such as façades and claddings, ceilings and walls, and roofs. Attributes include: anodizing free of streaks; color uniformity between produ.. |