Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 280 - 282 °C | 536 - 540 °F | Average value: 281 °C Grade Count:4 |
Overview of materials for Polyphenylene Sulfide (PPS); Molded This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS); Molded". Each property range of values reported is minimum and maximum valu.. |
|||
Melting Point | 260 - 282 °C | 500 - 540 °F | Average value: 277 °C Grade Count:6 |
Overview of materials for Polyphenylene Sulfide (PPS) with 30% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 30% Glass Fiber Filler". Specific grades with glass content between 25%.. |
|||
Melting Point | 280 - 282 °C | 536 - 540 °F | Average value: 281 °C Grade Count:3 |
Overview of materials for Polyphenylene Sulfide (PPS) with 50% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 50% Glass Fiber Filler". Specific grades with glass content between 45%.. |
|||
Melting Point | 252 - 282 °C | 485 - 540 °F | ASTM D-3418 |
Saint-Gobain Norton® FEP Fluoropolymer Film Features/Benefits:Outstanding clarityOutstanding anti-stick release propertiesPerformance from -254°C (-425°F) to 205°C (400°F)Exceptional chemical resistance and electric propertiesComp.. |
|||
Melting Point | 230 - 282 °C | 446 - 540 °F | |
Zeus ETFE Tubing ETFE (Ethylenetetrafluoroethylene), a copolymer of ethylene and tetrafluoroethylene, is used in applications requiring excellent impact, abrasion and stress cracking resistance. This polymer possess.. |