Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 174 - 184 °C | 345 - 363 °F | Average value: 177 °C Grade Count:9 |
Overview of materials for Nylon 12, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of .. |
|||
Melting Point | 180 - 184 °C | 356 - 363 °F | |
Suqian Unitechem Light Stabilizer 201 Product Name: Hydroxyethyl Piperidinol (HS-201)Chemical Name: 1-(2'hydroxyethyl)-2,2,6,6-Tetramethyl-4-piperidinolCAS NO.: 52722-86-8Molecular Formula: C11H23NO2Application: Tetramethyl piperidinol .. |
|||
Melting Point | 183 - 184 °C | 361 - 363 °F | |
Indium Corp. Indalloy 107 Tin-Lead Solder Alloy Information Provided by Indium Corporation |