Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 154 - 166 °C | 310 - 330 °F | MQSA 111 |
Lubrizol Advanced Materials PEARLCOAT® Activa D126K BL Thermoplastic Polyurethane Elastomer
(discontinued **) PEARLCOAT® Activa D126K BL is a standard polyester based TPU, supplied in form of translucent, black colored pellets, combining hardness with excellent low-temperature flexibility. PEARLCOAT® Acti.. |
|||
Melting Point | 158 - 166 °C | 316 - 331 °F | ASTM D3418 |
Solvay Specialty Polymers Solef® 5130 Polyvinylidene Fluoride (PVDF)
(Unverified Data**) Solef® 5130 PVDF has an ultra high viscosity ideal for its usage in lithium batteries.Additional Information: Intrinsic Viscosity: 0.27 - 0.37 l/gInformation provided by Solvay Specialty Polymers. |
|||
Melting Point | 163 - 166 °C | 325 - 331 °F | ASTM D3418 |
Arkema Group Kynar Flex® 3120 PVDF Copolymer
(discontinued **) Copolymer Series, Kynar® components are used extensively in the high purity semiconductor market, the pulp and paper industry, nuclear waste processing, and the general chemical processing industry.. |
|||
Melting Point | 162 - 166 °C | 324 - 331 °F | ISO 3146 |
Borealis Bormed™ DM55pharm Polypropylene Bormed™ DM55pharm is a low melt flow rate polypropylene homopolymer intended for extrusion and thermoforming. Its very good organoleptic properties allows this grade to be used with any master bat.. |
|||
Melting Point | 162 - 166 °C | 324 - 331 °F | DSC; ISO 3146 |
Borealis HB600TF Polypropylene HB600TF is a low melt flow rate polypropylene homopolymer intended for extrusion and thermoforming. Its very good organoleptic properties allows this grade to be used with any master batch without .. |
|||
Melting Point | 162 - 166 °C | 324 - 331 °F | DSC; ISO 3146 |
Borealis HC600TF Polypropylene HC600TF is a polypropylene homopolymer intended for thermoformed packaging applications. Its very good organoleptic properties allows this grade to be used with any masterbatch without discoloring .. |
|||
Melting Point | 162 - 166 °C | 324 - 331 °F | DSC; ISO 3146 |
Borealis HD204CF Polypropylene HD204CF is a homopolymer film resin, suitable for the manufacturing of unoriented film on chill roll process. Applications: HD204CF is recommended for medical applications, inner layer in co extru.. |
|||
Melting Point | 162 - 166 °C | 324 - 331 °F | DSC; ISO 3146 |
Borealis HD234CF Polypropylene HD234CF is a homopolymer film resin, suitable for the manufacturing of unoriented film on chill roll process. Applications: HD234CF is recommended for food packaging, lamination films, stationery f.. |
|||
Melting Point | 162 - 166 °C | 324 - 331 °F | DSC; ISO 3146 |
Borealis HD244CF Polypropylene HD244CF is a homopolymer film resin, suitable for the manufacturing of unoriented film on chill roll process. Applications: food packaging, lamination films, stationery folders, multi layer co-extr.. |
|||
Melting Point | 162 - 166 °C | 324 - 331 °F | DSC; ISO 3146 |
Borealis HD601CF Polypropylene HD601CF is a homopolymer film resin, suitable for the manufacturing of unoriented film on chill roll process. Applications: metallisable cast film, inner layer in co extrusion, textile packaging fil.. |
|||
Melting Point | 162 - 166 °C | 324 - 331 °F | DSC; ISO 3146 |
Borealis HD621CF Polypropylene HD621CF is a polypropylene homopolymer This grade is suitable for the manufacturing of unoriented films on cast and tubular quench film lines. Applications: food packaging, lamination films, statio.. |
|||
Melting Point | 162 - 166 °C | 324 - 331 °F | DSC; ISO 3146 |
Borealis HD214CF Polypropylene Homopolymer HD214CF is a homopolymer film resin, suitable for the manufacturing of unoriented film on chill roll process. Applications: food packaging, lamination films, stationary films, multi layer co-extrus.. |