Thermal Properties Metric English Comments
Melting Point 63.0 - 67.0 °C
145 - 153 °F
MQSA 70 A
Lubrizol Advanced Materials PEARLBOND® 121 Linear Thermoplastic Polyurethane
Pearlbondâ„¢ 121 is a linear, polycaprolactone-based polyurethane, supplied in form of small white granules, which combines an extremely high crystallization rate with a very high thermoplasticit..
Melting Point >= 63.0 °C
>= 145 °F
Hong Kun Group AO 1035 Antioxidant
Chemical Name: 2,2'-Thio-bis{ethyl-B-(3,5-ditertbutyl-4-hydroxyphenyl)}-propionateCAS No. 41484-35-9All information provided by Hongkun Group
Melting Point 63.0 - 67.0 °C
145 - 153 °F
MQSA 70 A
Lubrizol Advanced Materials PEARLBOND® 101 Linear Thermoplastic Polyurethane
Pearlbondâ„¢ 101 is a linear, polycaprolactone-based polyurethane, supplied in form of small white granules, which combines a very high crystallization rate with a very high thermoplasticity leve..
Melting Point 63.0 - 67.0 °C
145 - 153 °F
MQSA 70 A
Lubrizol Advanced Materials PEARLBOND® 501 Linear Thermoplastic Polyurethane
Pearlbondâ„¢ 501 is a linear, polycaprolactone-copolyester polyurethane, supplied in form of white spherical granules with a high crystallization rate and a very high thermoplasticity level.Appli..
Melting Point 63.0 °C
145 °F
ASTM D3417
DuPont Elvax® 150 Ethylene Vinyl Acetate
DuPont™ Elvax® 150 is an ethylene-vinyl acetate copolymer resin for use in industrial applications. Applications:Elvax® 150 resins can be used for the following applications: molding, compoundin..
Melting Point 63.0 °C
145 °F
ASTM D3417
DuPont Elvax® 150W Ethylene Vinyl Acetate
DuPont™ Elvax® 150W is an ethylene-vinyl acetate copolymer resin containing an anti-blocking additive for use in industrial applications. This resin is supplied in pellet form and to prevent the p..
Melting Point 63.0 °C
145 °F
ASTM D3418 - ISO 3146
DuPont Elvaloy® HP771 Ethylene/N-Butyl Acrylate/Carbon Monoxide Copolymer
Specialized copolymers deliver flexibility, toughness and weatherability to adhesives, plastics, highways and roofing.Availability: GloballyInformation provided by DuPont.
Melting Point 63.0 °C
145 °F
Freezing Point; ASTM D3418, ISO 3146
DuPont™ Elvax® 3155 Ethylene Vinyl Acetate
DuPont™ Elvax® 3155 is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins. ELVAX® 31..
Melting Point 63.0 °C
145 °F
Dow Method
Dow AFFINITY™ EG 8200G Ethylene alpha-olefin copolymer
AFFINITY™ EG 8200G Polyolefin Plastomer (POP) is produced via INSITE™ Technology from Dow Plastics. It exhibits high flexibility and elasticity. It can be utilized in monolayer cast film and in ..
Melting Point >= 63.0 °C
>= 145 °F
Wax Infiltrated; ASTM D3418
ALM PS 200 Prototyping Polymer
Non-spherical polystyrene powder for production of complex investment casting patterns.PS-200 can be used as a direct drop in replacement for Castform®, and can be successfully blended with Castfor..
Melting Point 63.0 °C
145 °F
DSC
Arkema Group EVATANE® 33-25 Copolymer Ethylene - Vinyl Acetate
EVATANE® 33-25 is a random copolymer of Ethylene and Vinyl Acetate made by high-pressure radicalar polymerisation process. EVATANE® 33-25 is stabilized with antioxidants. The High Vinyl Acetate co..
Melting Point >= 63.0 °C
>= 145 °F
Wax
3D Systems CastForm™ PS Plastic for SLS® Systems
For use with all selective laser sintering (SLS®) systems.ApplicationsCreate patterns directly rather than through indirect methodsComplex investment casting patternsReactive metals like titaniumLo..
Melting Point 63.0 - 67.0 °C
145 - 153 °F
MQSA 70 A
Lubrizol Advanced Materials PEARLBOND® 521 Linear Thermoplastic Polyurethane
Pearlbond™ 521 is a linear, polycaprolactone-copolyester polyurethane, supplied in form of white spherical granules with a very high crystallization rate and a very high thermoplasticity level.Appl..
Melting Point 63.0 °C
145 °F
ASTM D3417
DuPont Elvax® 150W-LG Ethylene Vinyl Acetate  (discontinued **)
DuPont™ Elvax® 150W-LG is an ethylene-vinyl acetate copolymer resin containing an anti-blocking additive for use in industrial applications. This resin is supplied in pellet form and to prevent th..