Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 58.0 - 60.0 °C | 136 - 140 °F | MQSA 70 A |
Lubrizol Advanced Materials PEARLBOND® DIPP-539 Linear Thermoplastic Polyurethane
(discontinued **) PEARLBOND® DIPP-539 is a linear, polycaprolactone-copolester polyurethane with a very high crystallization rate and a very high thermoplasticity level.Applications: PEARLBOND® DIPP-539 can be adde.. |
|||
Melting Point | 58.0 - 68.0 °C | 136 - 154 °F | |
Fine Organics FINALUX G 748 Lubricant Additive Applications: External lubricant and release agent for PVC, Polycarbonate, PET/PBT and ABS.Information provided by Fine Organics |
|||
Melting Point | 58.0 °C | 136 °F | |
LG Chemical LC170 Polyolefin Elastomer for Polymer Modification Features: Improved impact strength in polypropylene; Excellent filler acceptance; Available as pellet form; Outstanding toughness with flexible performance; and Reduction of product weightApplicatio.. |
|||
Melting Point | 58.0 °C | 136 °F | |
LG Chemical LC670 Polyolefin Elastomer for Polymer Modification Features: Improved impact strength in polypropylene; Excellent filler acceptance; Available as pellet form; Outstanding toughness with flexible performance; and Reduction of product weightApplicatio.. |
|||
Melting Point | 58.0 - 69.0 °C | 136 - 156 °F | |
Indium Corp. Indalloy 21 Bismuth Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 58.0 °C | 136 °F | Eutectic |
Indium Corp. Indalloy® 136 Bi-In-Pb-Sn Fusible Alloy General purpose fusible alloy. Wettability not outstanding. For use as solder.Information provided by the manufacturer, Indium Corporation. |
|||
Melting Point | 58.0 °C | 136 °F | Freezing point via DSC/ASTM D3418 |
DuPont Bynel® 3861 Anhydride-Modified Ethylene Vinyl Acetate Adhesive Resin Bynel® Series 3800 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p.. |
|||
Melting Point | 58.0 °C | 136 °F | |
BASF Ethylene Urea Formula: C3H6N2OCAS: 120-93-4Description: Ethylene urea is a colorless to yellow solid with a faint specific odor.Synonyms: 2-Imidazoleidinane, N,N’-Ethyleneurea, 2-Imidazolidone, 2-Oxoimidazolidin.. |
|||
Melting Point | 58.0 °C | 136 °F | |
AIM 58 Fusible Alloy Uses: lens blocking; proof casting; fusible element in safety devices; anchoring parts for machining; sealing adjustment screws; holding jet engine blades for machining and broaching; filler for sup.. |
|||
Melting Point | 58.0 - 60.0 °C | 136 - 140 °F | MQSA 70A |
Lubrizol Advanced Materials Pearlbond® 539 Thermoplastic Polyurethane Pearlbond® 539 is a linear, polycaprolactone-copolyester polyurethane, supplied in form of white spherical granules with a very high crystallization rate and a very high thermoplasticity level.Appl.. |