Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 548 - 660 °C | 1020 - 1220 °F | |
Materion AMC225XE T4 Aluminum/Silicon Carbide MMC Extruded Bar Aluminium alloy 2124 reinforced with 25 volume % silicon carbide particles (average size 3 micron). It is manufactured by a powder metallurgy route using high-energy mixing to ensure excellent part.. |
|||
Melting Point | 548 - 660 °C | 1020 - 1220 °F | |
Materion AMC225XE T4 Aluminum/Silicon Carbide MMC Forged Plate Aluminium alloy 2124 reinforced with 25 volume % silicon carbide particles (average size 3 micron). It is manufactured by a powder metallurgy route using high-energy mixing to ensure excellent part.. |
|||
Melting Point | >= 548 °C | >= 1020 °F | Solidus |
CRP Technology AMC225xe Aluminum Alloy - SiC Composite, T4 Condition AMC225xe is a high quality aerospace grade aluminum alloy (AA2124) reinforced with 25% by volume of ultrafine particles of silicon carbide. It is manufactured by a special powder metallurgy route us.. |