Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 268 - 286 °C | 514 - 547 °F | |
Williams Advanced Alloys WS286 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Melting Point | 268 - 290 °C | 514 - 554 °F | |
Williams Advanced Alloys WS290 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Melting Point | <= 268 °C | <= 514 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil HDPE HD 8760.29 High Density Polyethylene Resin Product Description: HD 8760 is a high density hexene copolymer designed to offer outstanding stiffness and processability. This resin is ideally suited for applications that require the optimum bal.. |
|||
Melting Point | <= 268 °C | <= 514 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil HDPE HD P8760.29 High Density Polyethylene Resin Product Description: HD 8760 is a high density hexene copolymer designed to offer outstanding stiffness and processability. This resin is ideally suited for applications that require the optimum bal.. |
|||
Melting Point | 268 - 299 °C | 514 - 570 °F | |
Johnson Matthey JM1090 Soft Solder/Flux General information on the Johnson Matthey soft solder and flux product line: A wide range of Tin/Lead solders suitable for a variety of applications is available from Johnson Matthey. Most materi.. |