Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 254 °C | 489 °F | ASTM D3418 |
Nylene® PA6/6 Glass Filled 5105 HS Nylon 6/6 5% Glass Filler; Property data for dry as molded samples.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation. |
|||
Melting Point | 254 °C | 489 °F | ASTM D3418 |
Nylene® PA6/6 Homopolymer 134 HSL Nylon 6/6 Low Viscosity Nucleated Grade; Property data for dry as molded samples.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation. |
|||
Melting Point | 254 °C | 489 °F | |
Ensinger ENSITEP® PBT Polybutylene Terephthalate - Extruded Products
(discontinued **) ENSITEP BT is an unreinforced thermoplastic polyester derived from polybutylene terephthalate. Its excellent wear and impact resistance, low coefficient of friction, high flexural modulus, and supe.. |
|||
Melting Point | 254 - 265 °C | 489 - 509 °F | Average value: 258 °C Grade Count:43 |
Overview of materials for Nylon 66, Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Bead Filled". Each property range of values reported is minimum and maximum values of ap.. |
|||
Melting Point | 254 °C | 489 °F | |
Shakespeare Resistat® F901 A013 Nylon 66 Monofilament Resistat F901, MERGE A013 is a .13 millimeter nylon 6,6 monofilament which has electrically conductive carbon suffused into the surface. The filament has a round cross section with a coating thickn.. |
|||
Melting Point | 254 °C | 490 °F | |
Techmer ES HiFill® PA6/6 CC20 Nylon 66 Availability: North AmericaForms: PelletsFiller/Reinforcement: Calcium Carbonate Filler, 20% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Melting Point | 254 °C | 489 °F | Typical Mylar® via DSC |
DuPont Teijin Films Mylar® EC Polyester Film, 200 Gauge Mylar® EC films are electrical grade films designed for use in applications where improved dimensional stability is required. In addition to lower levels of shrinkage, Mylar® EC films offer outsta.. |
|||
Melting Point | 254 °C | 489 °F | Typical Mylar® via DSC |
DuPont Teijin Films Mylar® EL21 Polyester Film, 1000 Gauge Mylar® EL21 polyester films are flexible strong and durable films with an unusual balance of properties, making them suitable for a variety of industrial applications. The excellent dielectric stre.. |
|||
Melting Point | 254 °C | 489 °F | Typical Mylar® via DSC |
DuPont Teijin Films Mylar® LJP Polyester Film, 275 Gauge Mylar® LJP is an industrial grade very clear film that is available with adhesion promoting coatings and slip coatings. For higher quality end-uses (especially for surface requirements) consider us.. |
|||
Melting Point | 254 °C | 489 °F | Typical Mylar® via DSC |
DuPont Teijin Films Mylar® M461 Polyester Film, 92 Gauge Mylar® M461 is a tough, general purpose, untreated polyester film. It is transparent in 48 through 300 gauge and translucent in heavier gauges. Mylar® M461 is based on DuPont Teijin Film's RSX fil.. |
|||
Melting Point | 254 °C | 489 °F | Typical Mylar® via DSC |
DuPont Teijin Films Mylar® MDA Polyester Film, 750 Gauge Mylar® MDA films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion.. |
|||
Melting Point | 254 °C | 489 °F | Typical Mylar® via DSC |
DuPont Teijin Films Mylar® OWF Polyester Film, 120 Gauge Product Description: Mylar® OWF is a co-extruded, one side amorphous, heat sealable polyester film designed to be used as an overwrap film. This film is suitable for use in contact with food. Appro.. |
|||
Melting Point | 254 °C | 489 °F | Typical Mylar® via DSC |
DuPont Teijin Films Mylar® RB42AF Polyester Film, 100 Gauge Product Description: Mylar® RB42AF is a biaxially oriented polyester (OPET) film with an ethylene vinyl acetate (EVA) heat seal layer and polyvinylidene chloride (PVdC) layer on the opposite side. .. |
|||
Melting Point | 254 °C | 489 °F | Typical Mylar® via DSC |
DuPont Teijin Films Mylar® RSX951 Polyester Film, 105 Gauge Mylar® RSX951 is a silicone coated polyester film designed for use as a release liner in various casting applications. The silicone release coating is applied to the film during the film production.. |
|||
Melting Point | 254 °C | 489 °F | Typical Mylar® via DSC |
DuPont Teijin Films Mylar® RSX951 Polyester Film, 92 Gauge Mylar® RSX951 is a silicone coated polyester film designed for use as a release liner in various casting applications. The silicone release coating is applied to the film during the film production.. |
|||
Melting Point | 254 °C | 489 °F | Typical Mylar® via DSC |
DuPont Teijin Films Mylar® WC Polyester Film, 48 Gauge Mylar® WC films are general-purpose electrical grade films, similar to Mylar® EL. These clear to hazy films are tough and durable as a core wrap. They offer good dielectrics and good handling char.. |
|||
Melting Point | 254 °C | 489 °F | ASTM D3418 |
E-Polymers Tekaster® F615GM , 40% GF/MF Reinforced PET 40% GF/MF Reinforced, Low warpageInformation provided by E-Polymers Co. Ltd. |
|||
Melting Point | 254 °C | 489 °F | Typical Mylar® via DSC |
DuPont Teijin Films Mylar® ADS Polyester Film, 200 Gauge Mylar® ADS is a heat stabilized, low shrinkage film with good web handling properties. Approvals: UL 94 VTM-2 - for 92 - 500 gauge (0.023 - 0.13mm)Also available in 285 GaugeInformation provided by.. |
|||
Melting Point | 254 °C | 489 °F | Typical Mylar® via DSC |
DuPont Teijin Films Mylar® LJP Polyester Film, 92 Gauge Mylar® LJP is an industrial grade very clear film that is available with adhesion promoting coatings and slip coatings. For higher quality end-uses (especially for surface requirements) consider us.. |
|||
Melting Point | 254 °C | 489 °F | Typical Mylar® via DSC |
DuPont Teijin Films Mylar® MDA Polyester Film, 48 Gauge Mylar® MDA films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion.. |
|||
Melting Point | 254 °C | 489 °F | ASTM D3418 |
E-Polymers Tekaster® F615G45 , 45% Glass Fiber Reinforced PET 45% Glass Fiber reinforced, High strength, Information provided by E-Polymers Co. Ltd. |
|||
Melting Point | 254 °C | 489 °F | ASTM D3418 |
Ashley Polymers Ashlene® E126WO PET Polyester, 30% Glass Reinforced PET Polyester with 30% glass reinforcement, flame retardant, natural. Note: Colors will modify properties.Data provided by the manufacturer |
|||
Melting Point | 254 °C | 489 °F | ASTM D789 |
Chem Polymer Chemlon 100 X Nylon 66, Lubricated GP A medium viscosity, general purpose injection molding grade nylon 66. Internally and externally lubricated for excellent feed and mold release properties.Data provided by the manufacturer, Chem Pol.. |
|||
Melting Point | 254 °C | 489 °F | ASTM D789 |
Chem Polymer Chemlon 109-18 G Nylon 66, 18% Glass Fiber Reinforced A highly toughened 18% glass fiber reinforced nylon 66 developed for applications requiring stiffness, creep resistance and impact resistance.Data provided by the manufacturer, Chem Polymer. |
|||
Melting Point | 254 °C | 489 °F | ASTM D789 |
Chem Polymer Chemlon 115 G Nylon 66, 15% Glass Fiber Reinforced A 15% glass fiber reinforced nylon 66 offering improved creep resistance, stiffness, tensile strength and dimensional stability over unmodified nylon 66 materials. This product offers slight improv.. |
|||
Melting Point | 254 °C | 489 °F | ASTM D789 |
Chem Polymer Chemlon 143 G Nylon 66, 43% Glass Fiber Reinforced A 43% glass fiber reinforced nylon 66 offering high rigidity and tensile strength, especially at high service temperatures.Data provided by the manufacturer, Chem Polymer. |
|||
Melting Point | 254 °C | 489 °F | ASTM D3418 |
Ashley Polymers Ashlene® 526 Nylon 66 High impact Nylon 66 with good stiffness and good low temperature properties for injection molding. Values shown are for Natural. Colors may change some properties.Data provided by the manufacture.. |
|||
Melting Point | 254 °C | 489 °F | ASTM D3418 |
Ashley Polymers Ashlene® 61M Nylon 66, 40% Mineral reinforced A 40% mineral reinforced general purpose Nylon 66 resin with superior stiffness and dimensional stability.Data provided by the manufacturer |
|||
Melting Point | 254 °C | 489 °F | Typical Mylar® via DSC |
DuPont Teijin Films Mylar® LJP Polyester Film, 300 Gauge Mylar® LJP is an industrial grade very clear film that is available with adhesion promoting coatings and slip coatings. For higher quality end-uses (especially for surface requirements) consider us.. |
|||
Melting Point | 254 °C | 489 °F | |
Shakespeare Resistat® F9116 A012 Nylon 66 Monofilament Resistat F9116, MERGE A012 is a 16 denier per filament nylon 6,6 chopped fiber. Each filament has electrically conductive carbon suffused into the surface. The filaments have a round cross section.. |