Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 244 °C | 471 °F | Crystalline Peak Melting Point; ASTM D3418 |
Eastman P76CC PET
(discontinued **) Voridian PET P76CC is used for dual ovenable containers and release paper.Applications/UsesDual ovenable containersRelease paper |
|||
Melting Point | >= 244 °C | >= 471 °F | WI No. 72A test |
Invista 1102 PET Copolymer Packaging Resin
(discontinued **) Carboxyl end groups: |
|||
Melting Point | 244 °C | 471 °F | |
Eastman Eastar EN058 PET Copolymer ISO data as provided by the manufacturer, Eastman Chemical |
|||
Melting Point | <= 244 °C | <= 471 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil Exceed™ 1518HA Metallocene Polyethylene Resin Product Description: Exceed 1518HA is a metallocene ethylene-hexene copolymer. Films made from Exceed 1518HA have outstanding tensile, impact strength and puncture. These superior strength propertie.. |
|||
Melting Point | <= 244 °C | <= 471 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil Exceed™ 2018CA Metallocene Polyethylene Resin (European Grade) Product Description: Exceed 2018CA is a metallocene ethylene-hexene copolymer. The higher melt index makes this polymer ideally suited for blending into LDPE rich films as well as skin layer in coex.. |
|||
Melting Point | <= 244 °C | <= 471 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil Exceed™ 2018EB Metallocene Polyethylene Resin (European Grade) Product Description: Exceed 2018EB is a metallocene ethylene-hexene copolymer. The higher melt index makes this polymer ideally suited for blending into LDPE rich films. Availability: Africa & Middl.. |
|||
Melting Point | <= 244 °C | <= 471 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil Exceed™ 2018KB Metallocene Polyethylene Resin (European Grade) Product Description: Exceed 2018KB is a metallocene catalyzed ethylene-hexene copolymer. Films made from Exceed 2018KB have outstanding tensile, impact strength, and puncture. These superior strengt.. |
|||
Melting Point | 244 °C | 471 °F | nominal; DAK-QAR-SOP-0016 |
DAK Americas Laser+® C91A PET Product Description: Laser+® (C91A) polyethylene terephthalate (PET) resin is a copolymer formulated for conversion to PET bottles by conventional single or two-stage processing technology.Typical .. |
|||
Melting Point | 244 °C | 471 °F | nominal; DAK-QAR-SOP-0016 |
DAK Americas Laser+® HS CF746A (D53A) PET Product Description: Laser+® HS CF746A (D53A) polyethylene terephthalate (PET) resin is designed for conversion to PET packaging by injection stretch blow-molding using commercial heat-set technolo.. |
|||
Melting Point | 244 °C | 471 °F | nominal; DAK-QAR-SOP-0016 |
DAK Americas Laser+® W 4000 K42A PET Product Description: Laser+® W 4000 (K42A) polyethylene terephthalate (PET) resin is a copolymer formulated for conversion to PET bottles by conventional single or two-stage processing technology.T.. |
|||
Melting Point | <= 244 °C | <= 471 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil Exceed™ 1018EB Metallocene Polyethylene Resin (European Grade) Product Description: Exceed 1018EB is a metallocene ethylene-hexene copolymers. Films are made of Exceed 1018EB have outstanding tensile, impact, puncture resistance and low temperature properties. .. |
|||
Melting Point | 244 °C | 471 °F | ISO 11357 |
Ascend Performance Materials Vydyne® 85XFS Nylon 66/6, General Purpose Vydyne® 85XFS is a general-purpose PA66/6 resin. It is available in natural and is designed for extrusion-compounding applications. This copolymer PA66/6 resin provides a lower melting point and ca.. |
|||
Melting Point | 244 °C | 471 °F | ISO 11357-3 |
Ascend Performance Materials Vydyne® ECO315 BK06 Nylon 66/6, Flame Retardant, DAM Vydyne® ECO315 BK06 is a non-halogenated, unfilled, flame-retardant PA66/6 copolymer with excellent toughness and ductility. It is lubricated for machine feed and easy mold release and has Underwri.. |
|||
Melting Point | 244 °C | 471 °F | ISO 11357-3 |
Ascend Performance Materials Vydyne® ECO-315 Nylon 66/6, non-halogenated, ignition resistant, DAM Vydyne® ECO315 is non-halogenated, unfilled, flame-retardant PA66/6 copolymer with excellent strength and toughness. It is lubricated for machine feed and has an Underwriters Laboratories UL 94 fla.. |
|||
Melting Point | 244 - 255 °C | 471 - 491 °F | Average value: 250 °C Grade Count:15 |
Overview of materials for Polyethylene Terephthalate (PET), 50% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 50% Glass Reinforced". Specific grades with glass content between 45% .. |
|||
Melting Point | <= 244 °C | <= 471 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil Exceed™ 1018CA Metallocene Polyethylene Resin (European Grade) Product Description: Exceed 1018 CA is a metallocene ethylene-hexene copolymers. Films are made of Exceed 1018CA have outstanding tensile, puncture resistance and very good sealing properties. These.. |