Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 240 °C | 464 °F | |
Omnia Plastica Akulon® PA 66.6 - Akulon GX - at 50% RH Copolymer of nylon with excellent mechanical features, it combines the good impact resistances of PA6 as well as the higher stiffness of PA66. For this reason it machines very well on automatic tool.. |
|||
Melting Point | 240 °C | 464 °F | ISO 11357-3 |
Pasargad Polymer Peyvand Pasadur 3P-H8130B PBT, 30% Glass Fiber Reinforced Form: PelletsProcessing Method: Injection MoldingUses: Automotive Application Furniture Appliance Components Automotive Exterior PartsAutomotive Interior PartsInformation provided by Pasargad Poly.. |
|||
Melting Point | 240 °C | 464 °F | ISO 11357-3 |
Pasargad Polymer Peyvand Pasalac 3P-H6000B ABS Form: PelletsProcessing Method: Injection MoldingUses: Automotive Application Furniture Appliance Components Automotive Exterior PartsAutomotive Interior PartsInformation provided by Pasargad Poly.. |
|||
Melting Point | 240 °C | 464 °F | |
Plastcom SLOVASTER® C FRU 2 PBT, flame retarder FeaturesPC with the flame retardant on the basis of bromine hydrocarbons. Anisotropy of shrinkage enables the injection moulding of round, cylindrical or other hole products. Application in engineer.. |
|||
Melting Point | 240 °C | 464 °F | Crystalline Peak Melting Point; ASTM D3418 |
Eastman 9921 PET Film
(discontinued **) VORIDIAN polymer 9921 is a copolymer PET that has been crystallized. Color concentrates of polymer 9921 are available on request.Applications/UsesAutomotive parts containersFood packagingHousehold p.. |
|||
Melting Point | 240 °C | 464 °F | |
Eastman Eastalloy DA105 PC+PET Copolyester/Polycarbonate
(discontinued **) ISO data as provided by the manufacturer, Eastman Chemical |
|||
Melting Point | 240 °C | 464 °F | crystalline melting point; ASTM D4591 |
Honeywell Halar® High Performance E-CTFE Film
(discontinued **) Description: Halar® is a high performance Ethylene-Chlorotrifluoroethylene (E-CTFE) film with excellent mechanical, electrical and release properties. It is non-flammable, and has outstanding chem.. |
|||
Melting Point | 240 °C | 464 °F | Target; M2E-73-002 |
Indorama Ventures Mexico Polyclear™ Plus 1111 PET Resin Description: La resina Polyclear® Plus PET 1111 de Arteva Specialties, es un copolimero para empaque con una viscosidad intrinseca de 0.84 dl/g. Los envases fabricados con este material tienen un.. |
|||
Melting Point | 240 °C | 464 °F | ASTM D-3418 |
Saint-Gobain Norton® PMP Film Features/Benefits:Good release properties for up to 180°C (356°F) cure composites (application dependent)low density for high surface area per poundExcellent clarityThermoformableProduct avail.. |
|||
Melting Point | >= 240 °C | >= 464 °F | |
Wellman PermaClear™ 61803 (0.81 IV) PET PermaClear® 61803 is a TPA-based polyethylene terephthalate resin made especially for use in packaging applications. It is a solid-stated copolymer resin with an intrinsic viscosity 0.81 IV. PermaC.. |
|||
Melting Point | >= 240 °C | >= 464 °F | BD-61305 |
Wellman PermaClear™ HP806 (0.84 IV) PET PermaClear® HP806 is a TPA-based polyethylene terephthalate resin made especially for use in packaging applications. It is a solid-stated copolymer resin with an intrinsic viscosity 0.84 IV. PermaC.. |
|||
Melting Point | 240 °C | 464 °F | BD-61305 |
Wellman ThermaClear® Ti818 (0.79 IV) PET ThermaClearTI® Ti818 is a TPA-based polyethylene terephthalate resin made especially for use in packaging applications. Its titanium catalyst and copolymer formulation provide outstanding clarity a.. |
|||
Melting Point | 240 °C | 464 °F | DSC |
Westlake Plastics ECTFE Film Made from HALAR® Ethylene-chlorotrifluoroethylene Resin Excellent purity. Excellent chemical resistance. Low permeability. Excellent abrasion resistance. Excellent temperature resistance.Halar® is a trade name of Solvay Solexis, Inc. Information p.. |
|||
Melting Point | 240 °C | 464 °F | Crystalline Peak Melting Point; ASTM D3418 |
Eastman Aqua PJ003 PET Voridian Aqua PET PJ003 is a condensation polymer produced by a continuous melt-phase polymerization process followed by a solid-state polymerization process. This product is specifically designed f.. |
|||
Melting Point | 240 °C | 464 °F | nominal; DAK-QAR-SOP-0016 |
DAK Americas Laser+® HP806 (B93A) PET Product Description: Laser+® HP806 (B93A) polyethylene terephthalate (PET) resin is a copolymer formulated for conversion to PET bottles by conventional single or two-stage processing technology.Ty.. |
|||
Melting Point | 240 °C | 464 °F | nominal; DAK-QAR-SOP-0016 |
DAK Americas Laser+® W PJ002 F43A PET Product Description: Laser+® W PJ002 (F43A) polyethylene terephthalate (PET) resin is a copolymer formulated for conversion to PET bottles by conventional single or two-stage processing technology... |
|||
Melting Point | >= 240 °C | >= 464 °F | |
Ex-Tech Plastics VersaTech™ APET Ex-Tech VersaTech™ APET has exceptional properties such as visual transparency high heat distortion and it has good resistance to mineral oils, solvents and acids.Characteristics:TransparentExcepti.. |
|||
Melting Point | 240 °C | 464 °F | DIN 53765 |
BASF Ultramid® C3U10 BK 23079 PA6/66 FR (Conditioned) Description: Flame-retardant injection-molding grade; light colorable. Burning behavior optimized for glow-wire requirements of IEC 60335. Typical applications are switches, housings, plug connector.. |
|||
Melting Point | 240 °C | 464 °F | |
Asahi Glass Fluon® AH-2000 LM-ETFE, Non-Conductive Type, Fluororesin Fluon®LM-ETFE AH series is a fluoro-resin which have an adhesive properties, and is possible to adhere with other materials by melting down. It can be applied directly without privilege adhesive ag.. |
|||
Melting Point | 240 °C | 464 °F | |
Asahi Glass Fluon® AH-3000 LM-ETFE, Conductive Type, Fluororesin Fluon®LM-ETFE AH series is a fluoro-resin which have an adhesive properties, and is possible to adhere with other materials by melting down. It can be applied directly without privilege adhesive ag.. |
|||
Melting Point | 240 °C | 464 °F | MPC Method |
Mitsui TPX® MX004 Methylpentene Copolymer TPX® is a 4-methylpentene-1 based polyolefin with a unique combination of transparency, heat and chemical resistant qualities. TPX is used in a wide variety of applications, including: medical equi.. |
|||
Melting Point | 240 °C | 464 °F | MPC Method |
Mitsui TPX® RT18 Methylpentene Copolymer, Transparent Grade TPX® is a 4-methylpentene-1 based polyolefin with a unique combination of transparency, heat and chemical resistant qualities. TPX is used in a wide variety of applications, including: medical equi.. |
|||
Melting Point | 240 °C | 464 °F | MPC Method |
Mitsui TPX® RT18 XB Methylpentene Copolymer TPX® is a 4-methylpentene-1 based polyolefin with a unique combination of transparency, heat and chemical resistant qualities. TPX is used in a wide variety of applications, including: medical equi.. |
|||
Melting Point | 240 °C | 464 °F | |
Solvay Specialty Polymers Ixef® 1313/0004 Polyarylamide, 40% Glass Fiber + Elastomer, DAM
(discontinued **)&l Impact modified. The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manu.. |
|||
Melting Point | 240 °C | 464 °F | |
Solvay Specialty Polymers Ixef® 1313/0004 Polyarylamide, 40% Glass Fiber + Elastomer, at Equilibrium (65% RH)
  Impact modified. The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manu.. |
|||
Melting Point | 240 °C | 464 °F | |
Solvay Specialty Polymers Ixef® 2010/X914 Polyarylamide, 40% Filler, DAM
(discontinued **) The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A.. |