Polymer Property : Melting Point = 235 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 235 °C
455 °F
ASTM D3418
Nylene® 6111 (HS) , 40% Glass/Mineral Reinforced Nylon 6/6
Description: Nylene® 6111 (HS) is a 40% mineral reinforced, impact modified nylon 6/6. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Pol..
Melting Point 235 °C
455 °F
ASTM D3418
Nylene® 9633 , 33% Glass Reinforced Nylon 6,6/6
Description: Nylene® 9633 is a 33% glass fiber reinforced specialty nylon. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resou..
Melting Point 235 °C
455 °F
ASTM D3418
Nylene® 9643 , 43% Glass Reinforced Nylon 6,6/6
Description: Nylene® 9643 is a 43 % glass fiber reinforced specialty nylon. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Reso..
Melting Point 235 - 310 °C
455 - 590 °F
Average value: 258 °C Grade Count:38
Overview of materials for Nylon 66/6, 40% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 40% Glass Fiber Reinforced". Specific grades with glass content between 35% and 44% are incl..
Melting Point 235 - 263 °C
455 - 505 °F
Average value: 254 °C Grade Count:9
Overview of materials for Nylon 66/Nylon 6 Blend, Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/Nylon 6 Blend, Glass Fiber Filled". Each property range of values reported is minimum and maxim..
Melting Point 235 - 240 °C
455 - 464 °F
Indium Corp. Indalloy® 133 Sn-Sb Solder Alloy
Higher tensile strength solder than #121. Particular application is joining copper tubing in refrigeration and potable water systems. Has good wettability with good long time sheer strength at 100Â..
Melting Point 235 - 245 °C
455 - 473 °F
Sheath Melt Point; LCL-PR29
Intercontinental Polymers 1613 Bicomponent PBN/PET Fiber Type - 1.8 Denier X 3.0 Inches
50/50 PBN Sheath/PET Core. Luster: Semi-Dull. Finish: Hydrophilic.Applications of bicomponent polyester fiber: Absorbent products, hygiene products, non-wovens, filtration, sliver knit, microdenie..
Melting Point 235 °C
455 °F
DSC
Westlake Plastics PMP Film Made from TPX® Polymethylpentene Resin
Lowest specific gravity of any known thermoplastic. Exceptional electrical properties. Good chemical resistance. High heat resistance. Excellent acoustical properties. Transparency. FDA compli..
Melting Point 235 °C
455 °F
Williams Advanced Alloys WS235 Solder
All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys
Melting Point 235 °C
455 °F
10°C/min; ISO 11357-1/-3
EMS-Grivory Grivory® G4V-5H black 9915 PA*-GF50
Product description: Grivory G4V-5H is a 50% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline partially aromatic copolyamide. Grivory G4V-5H is used for injectio..
Melting Point 235 °C
455 °F
10°C/min; ISO 11357-1/-3
EMS-Grivory Grivory® G4V-5H nat PA*-GF50
Product description: Grivory G4V-5H is a 50% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline partially aromatic copolyamide. Grivory G4V-5H is used for injectio..
Melting Point <= 235 °C
<= 455 °F
Peak Melting Point; ExxonMobil method
ExxonMobil LDPE LD 071.LQ Low Density Polyethylene Resin
Product Description: LD 071 Series case wrap film resins combine good processability with excellent strength and good film optics for bundling applications requiring proper shrink performance, tough..
Melting Point <= 235 °C
<= 455 °F
Peak Melting Point; ExxonMobil method
ExxonMobil LDPE LD 071.LR Low Density Polyethylene Resin
Product Description: LD 071 Series case wrap film resins combine good processability with excellent strength and good film optics for bundling applications requiring proper shrink performance, tough..
Melting Point <= 235 °C
<= 455 °F
Peak Melting Point; ExxonMobil method
ExxonMobil LDPE LD 156BW Low Density Polyethylene Resin
Product Description: LD 156 series are LDPE grades, specially designed for lamination films and co-extruded films. They offer good mechanical, stiffness and optical properties, combined with very lo..
Melting Point <= 235 °C
<= 455 °F
Peak Melting Point; ExxonMobil method
ExxonMobil LDPE LD 156HE Low Density Polyethylene Resin
Product Description: LD 156 series are LDPE grades, specially designed for lamination films and co-extruded films. They offer good mechanical, stiffness and optical properties, combined with very lo..
Melting Point 235 °C
455 °F
ISO 11357-3
Ascend Performance Materials Vydyne® 86XFS Nylon 66/6
Vydyne® 86XFS is a medium-viscosity PA66/6 random copolymer used for extrusion-compounding. This copolymer is specifically designed to be used with FR packages and high mineral loadings due to its ..
Melting Point 235 °C
455 °F
ASTM D789
Aclo Accucomp Nylon 6 NY0700L
Melting Point 235 °C
455 °F
ISO 11357-1/-2
BASF Ultradur® B 4040 G10 50% Glass Filled BK 15029 PBT + PET
Description: Injection molding grade with 50% glass fibers for industrial parts with excellent surface quality, for example external door handles in vehicles, visible sunroof frames, oven door handl..
Melting Point 235 °C
455 °F
10K/min; ISO 3146
CENTROPLAST CENTROSOL Acrylonitrile butadiene Styrene copolymer
CENTROSOL ABS has high rigidity and hardness even at low temperatures. It is scratch resistant, non-toxic, with high surface resistance. It is used in operation components for electrical equipment ..
Melting Point 235 °C
455 °F
MPC Method
Mitsui TPX® MX002 Methylpentene Copolymer
TPX® is a 4-methylpentene-1 based polyolefin with a unique combination of transparency, heat and chemical resistant qualities. TPX is used in a wide variety of applications, including: medical equi..