Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 161 °C | 322 °F | |
Hyosung Topilene J351F PP J351F Block CopolymerApplications: Retort CPPCharacteristics:Excellent impact strengthFish eye freeHeat resistanceGood clarityInformation provided by Hyosung Corporation |
|||
Melting Point | 161 °C | 322 °F | |
Hyosung Topilene J440F PP J440F Block CopolymerApplications: Retort CPPCharacteristics:Excellent impact strengthFish eye freeHeat resistanceGood clarityInformation provided by Hyosung Corporation |
|||
Melting Point | 161 °C | 322 °F | DSC |
Silon Tabond 5010 Adhesive Resin Tabond 5010 is a a chemically modified Polypropylene. This grade is for sheets and bottles composed of Polypropylene (PP) and EVOH or PA.Characteristics: • Strong adhesion to PA / PP and EVOH /.. |
|||
Melting Point | 161 - 165 °C | 322 - 329 °F | ISO 3146 |
Borealis Borclean™ HB300BF Polypropylene Homopolymer for Capacitor Film Borclean HB300BF is a homopolymer film resin developed for use in the manufacture of the highest quality films or dielectric applications. Borclean HB300BF does not contain slip, antiblock, antista.. |
|||
Melting Point | 161 - 165 °C | 322 - 329 °F | ISO 3146 |
Borealis Borclean™ HB311BF Polypropylene Homopolymer for Capacitor Film Borclean HB311BF is a homopolymer film resin developed for use in the manufacture of the highest quality films for dielectric applications. Borclean HB311BF does not contain slip, antiblock, antist.. |
|||
Melting Point | 161 - 165 °C | 322 - 329 °F | ISO 3146 |
Borealis Borclean™ HC300BF Polypropylene Homopolymer for Capacitor Film Borclean HC300BF is a homopolymer film resin developed for use in the manufacture of the highest quality films for dielectric applications. Borclean HC300BF does not contain slip, antiblock, antist.. |
|||
Melting Point | 161 - 165 °C | 322 - 329 °F | ISO 3146 |
Borealis Borclean™ HC312BF Polypropylene Homopolymer for Capacitor Film Borclean HC312BF is a homopolymer film resin developed for use in the manufacture of the highest quality films for dielectric applications. Borclean HC312BF does not contain slip, antiblock, antist.. |
|||
Melting Point | 161 - 165 °C | 322 - 329 °F | ISO 3146 |
Borealis Borclean™ HC314BF Polypropylene Homopolymer for Capacitor Film Borclean HC314BF is a homopolymer film resin developed for use in the manufacture of the highest quality films for dielectric applications. Borclean HC314BF does not contain slip, antiblock, antist.. |
|||
Melting Point | 161 - 165 °C | 322 - 329 °F | ISO 3146 |
Borealis Borclean™ HC318BF Polypropylene Homopolymer for Capacitor Film Borclean HC318BF is a homopolymer film resin developed for use in the manufacture of the highest quality films for dielectric applications. Borclean HC318BF does not contain slip, antiblock, antist.. |
|||
Melting Point | 161 - 165 °C | 322 - 329 °F | ISO 3146 |
Borealis Borclean™ HC320BF Polypropylene Homopolymer for Capacitor Film Borclean HC320BF is a homopolymer film resin developed for use in the manufacture of the highest quality films for dielectric applications. Borclean HC320BF does not contain slip, antiblock, antist.. |
|||
Melting Point | 161 - 165 °C | 322 - 329 °F | ISO 3146 |
Borealis Borflow™ HL504FB Polypropylene Homopolymer Borflow HL504FB is a polypropylene homopolymer grade intended for fiber applications characterized by narrow molecular weight distribution, controlled rheology, easy processability, optimal product .. |
|||
Melting Point | 161 - 165 °C | 322 - 329 °F | DSC; ISO 3146 |
Borealis HC101BF Polypropylene Homopolymer HC101BF is a polypropylene homopolymer. Applications: HC101BF has been developed especially for applications like: co-extrusion applications, print lamination, metallisable film, coated film, packa.. |
|||
Melting Point | 161 - 165 °C | 322 - 329 °F | ISO 3146 |
Borealis HF420FB Polypropylene HF420FB is a polypropylene homopolymer intended for fiber applications. HF420FB has been developed especially for applications like: staple fiber, continuous filaments, and spun bonded nonwovens.In.. |
|||
Melting Point | 161 - 165 °C | 322 - 329 °F | DSC; ISO 3146 |
Borealis HG265FB Polypropylene HG265FB is a polypropylene homopolymer intended for fiber applications. Applications: bulked continuous filaments, staple fiber for nonwoven, staple fiber for textiles, and continuous filaments. A.. |
|||
Melting Point | 161 - 165 °C | 322 - 329 °F | DSC; ISO 3146 |
Borealis HG420FB Polypropylene HG420FB is a polypropylene homopolymer intended for fiber applications. Applications: HG420FB has been developed especially for applications like spun bonded nonwovens.Information provided by Borea.. |
|||
Melting Point | 161 - 165 °C | 322 - 329 °F | ISO 3146 |
Borealis HG455FB Polypropylene Homopolymer HG455FB is a polypropylene homopolymer intended for fiber applications. Applications: fine filament count at high spinning speeds, spun bonded nonwovens, and POY production.Information provided by .. |
|||
Melting Point | 161 - 165 °C | 322 - 329 °F | ISO 3146 |
Borealis HH450FB Polypropylene Homopolymer HH450FB is a polypropylene homopolymer intended for fiber applications. Applications: HH450FB has been developed especially for applications like spunbonded nonwovens.Information provided by Boreal.. |
|||
Melting Point | 161 °C | 322 °F | DSC |
Lubrizol ESTANE® ETE60DT3 Ester Based Thermoplastic Polyurethane Features: Hard TPU with wide extrusion processing window and melt stability, low temperature flexibility, high transparency, UV stableUses: Extrusion: Hose and Tube, Extrusion: Profile, Cable Jacket.. |
|||
Melting Point | 161 - 165 °C | 322 - 329 °F | DSC; ISO 3146 |
Borealis HE365FB Polypropylene HE365FB is a polypropylene homopolymer intended for fiber applications. Applications: continuous filaments, and staple fiber. HE365FB Gas fading free formulation contains antioxidant and UV stabil.. |
|||
Melting Point | 161 °C | 322 °F | DSC; Dow Method |
Dow DX5E66 Polypropylene Homopolymer Resin OverviewConsistent processabilityVery high cleanlinessGood optical propertiesComplies with U.S. FDA 21 CFR 177.1520 (c)1.1a, EU-Directive 2002/72/EC, Canadian HPFB No ObjectionDX5E66 Developmental P.. |
|||
Melting Point | 161 °C | 322 °F | DSC; Dow Method |
Dow H110-02N Polypropylene Homopolymer Resin OverviewContains a nucleating agentHigh clarityGood melt strengthComplies with U.S. FDA 21 CFR 177.1520 (c)3.2a, Canadian HPFB No ObjectionDOW H110-02N Polypropylene Resin is intended for use in ext.. |
|||
Melting Point | 161 °C | 322 °F | Dow Method (DSC) |
Dow H110-02N Polypropylene Resin DOW H110-02N is intended for use in extrusion and thermoforming processes. It is especially suited for applications where improved melt strength and clarity are desired.Information provided by DowD.. |
|||
Melting Point | 161 °C | 322 °F | |
Arkema Group Orevac® 18732 RBP Maleic Anhydride modified Polypropylene PP base Structure: Repairing and joint Applications: Pipe CoatingInformation provided by Arkema Group |
|||
Melting Point | 161 °C | 322 °F | 10°C/min |
Arkema Group Appryl® CZN 0525 Polypropylene, 25% Talc Filled Compound of a PP copolymer modified with EPR and 25% talc. This grade has been specially developed for interior trim applications, that required an excellent impact test associated with a high modul.. |
|||
Melting Point | 161 - 168 °C | 322 - 334 °F | |
Arkema Group KYNAR FLEX® 3120-15 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, flame and smoke suppressant. High stability in harsh thermal, chemical and ultraviolet environments. High toughness.. |
|||
Melting Point | 161 - 168 °C | 322 - 334 °F | |
Arkema Group KYNAR FLEX® 3120-50 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, 150°C temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness a.. |
|||
Melting Point | 161 °C | 322 °F | 10°C/min |
Arkema Group Appryl® CZU 0525 Polypropylene, 25% Talc Filled Compound of a PP copolymer modified with EPR and 25% talc. This grade has been specially developed for exterior trim automotive applications, that required an excellent impact test associated with a.. |
|||
Melting Point | 161 - 165 °C | 322 - 329 °F | DSC; ISO 3146 |
Borealis HE465FB Polypropylene HE465FB is a polypropylene homopolymer intended for fiber applications. Applications: high tenacity CF yarn. Additives: HE465FB gas fading free formulation.Information provided by Borealis AG |
|||
Melting Point | 161 °C | 322 °F | DSC; Dow Method |
Dow H110-02NZ Polypropylene Homopolymer Resin OverviewContains a nucleating agentGood melt strengthComplies with U.S. FDA 21 CFR 177.1520 (c)3.2aDOW H110-02NZ Polypropylene Resin is intended for use in extrusion and thermoforming processes in o.. |