Thermal Properties Metric English Comments
Melting Point 148 - 155 °C
298 - 311 °F
Pau Tai Calcium stearate, Monomer Stabilizer
Non sulfide staining and non-toxic. Excellent internal lubricity and good gelation property.Applications: Hard products, non-toxic adhesive plaster and rubber mold release
Melting Point 148 °C
298 °F
DSC
Solvay Specialty Polymers Solef® 20808 Polyvinylidene Fluoride (PVDF)
Copolymer; Low ViscosityAdditional Properties: Abrasion Resistance - ASTM D4060 29.0 mg; Coefficient of Friction - ASTM D1894 0.280; Coefficient of Linear Thermal Expansion - ASTM D696 1.4E-4 to 1.6..
Melting Point 148 - 154 °C
298 - 309 °F
DSC; ISO 3146
Borealis BorPure™ RD234CF Polypropylene Random Copolymer
BorPure™ RD234CF is a random copolymer. This grade is suitable for the manufacturing of unoriented films on chill roll processes. Applications: RD234CF is recommended for food packaging, stationa..
Melting Point 148 - 154 °C
298 - 309 °F
DSC; ISO 3146
Borealis RD204CF Polypropylene Random Copolymer
RD204CF is a random copolymer. This grade is suitable for the manufacturing of unoriented films on chill roll processes. Applications: RD204CF is recommended for blending, food packaging, high qua..
Melting Point 148 - 154 °C
298 - 309 °F
DSC; ISO 3146
Borealis RD461CF Polypropylene Random Copolymer
RD461CF is a random copolymer. This grade is suitable for the manufacturing of unoriented films on chill roll processes. Applications: RD461CF is recommended for food packaging, high quality stati..
Melting Point 148 - 154 °C
298 - 309 °F
DSC; ISO 3146
Borealis RD734CF Polypropylene Random Copolymer
RD734CF is a random copolymer. This grade is suitable for the manufacturing of unoriented films on chill roll processes. Applications: RD734CF is recommended for food packaging, high quality stati..
Melting Point 148 °C
298 °F
DSC
Total PPR 6573XHC Polypropylene, Random Copolymer Film Grade
Random copolymer film gradeColor - Low catalyst residuals in FINA 6573XHC result in improved color stability.Clarity/Impact - The random copolymer structure of FINA 6573XHC improves its clarity and ..
Melting Point 148 °C
298 °F
DSC
Total PPR 6575 Polypropylene, Random Copolymer, Film Grade
Color. Low catalyst residuals in TOTAL Petrochemicals 6575 polypropylene results in improved color stability.Clarity/Impact. The random copolymer structure of 6575 improves its clarity and resilien..
Melting Point 148 °C
298 °F
DSC; ASTM D3417
Dow 6D20 Polypropylene Random Copolymer Resin
OverviewConsistent processabilityGood regrind stabilityGood gloss and clarityLow odor and taste transferComplies with: U.S. FDA 21 CFR 177.1520 (c)3.1a, Europe EU-Directive 2002/72/ECDOW 6D20 Polypr..
Melting Point 148 °C
298 °F
Dow Method (DSC)
Dow 6D20 Polypropylene Resin
DOW 6D20 is intended for use in film and extrusion blow molding processes. It is especially suited for multilayered, barrier bottles.Information provided by DowDow Announced Sale of Global Polyprop..
Melting Point 148 °C
298 °F
DSC; Dow Method
Dow R131-02A Polypropylene Random Copolymer Resin
DOW R131-02A Polypropylene Resin is a random copolymer intended for use in extrusion blow molding applications. The product can be used in both single layer and multilayer designs including barrier..
Melting Point 148 °C
298 °F
DSC; Dow Method
Dow R132-02A Polypropylene Random Copolymer Resin
DOW R132-02A Polypropylene Resin is a random copolymer intended for use in extrusion blow molding applications. The product can be used in both single layer and multilayer designs including barrier..
Melting Point 148 °C
298 °F
ISO 11357
Arkema Group Pebax® Rnew 40R53 SP 01 Polyether Block Amide (PEBA)
Polyether block amide Pebax® 40R53 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide based on renewable resources. This SP grade has been developed to be heat and UV..
Melting Point 148 - 149 °C
298 - 300 °F
AIM 80In/Pb15/Ag5 Solder for Photonic Packaging
Uses include:Fiber to Ferrule SolderingLaser Die AttachHermetic Packaging & SealingWetting & Sealing Laser OpticsThermal ManagementInformation provided by AIM Specialty Materials.
Melting Point 148 - 152 °C
298 - 306 °F
Arkema Group KYNAR® LBG1 Polyvinylidene Fluoride Powder
Characteristics: White, non-hygroscopic powder.Applications: Membrane, Lithium ion battery applicationsInformation provided by Arkema Inc.
Melting Point 148 °C
298 °F
ISO 3146
Total PPR 3260 Random Copolymer Polypropylene, Extrusion Grade
Polypropylene PPR 3260 is a random copolymer polypropylene with a melt flow index of 1.8 g/10 min suitable for extrusion applications.Information provided by Total Petrochemicals.