Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 143 °C | 289 °F | |
Hyosung Topilene C600Y PP C600Y Butene Random CopolymerApplications: FilmCharacteristics:Excellent transparency & glossLow sealing temperatureHigh hot-tack strengthGood stiffnessInformation provided by Hyosung Corporation |
|||
Melting Point | 143 - 237 °C | 289 - 459 °F | |
Indium Corp. Indalloy® 3 In-Ag Solder Alloy Has nearly the wettability and low temperature malleability of Indium. Solders silver, fired glass, and ceramics. Large plastic range.Information provided by the manufacturer, Indium Corporation. |
|||
Melting Point | 143 °C | 289 °F | Eutectic |
Indium Corp. Indalloy® 290 In-Ag Solder Alloy Indium with silver added to improve strength. Has the wettability and low-temperature malleability of indium. Particularly useful for cryogenic applications.Information provided by the manufacturer,.. |
|||
Melting Point | 143 - 154 °C | 290 - 310 °F | MQSA 111 |
Lubrizol Advanced Materials PEARLCOAT® 162K Thermoplastic Polyurethane Elastomer PEARLCOAT® 162K is a polyether based TPU, supplied in form of translucent, colorless pellets, combining hardness with excellent low temperature flexibility and very good hydrolysis resistance. PE.. |
|||
Melting Point | 143 °C | 289 °F | DSC |
Shakespeare Isocorâ„¢ TT65SI Nylon 6 Terpolymer Isocorâ„¢ TT65SI multi-polymer is a linear polyamide with unique solubility characteristics and physical properties. Unlike conventional polyamides, Isocorâ„¢ TT65SI is soluble in common al.. |
|||
Melting Point | 143 °C | 289 °F | DSC |
Silon Tabond 5009 Adhesive Resin Tabond 5009 is a chemically modified Polypropylene. This grade is for coextrusion coating of multilayer film to give adhesion between the layers.Characteristics: • Strong adhesion to Aluminium .. |
|||
Melting Point | 143 - 147 °C | 289 - 297 °F | ISO 3146 |
Borealis Borclear™ RB707CF Polypropylene Random Copolymer for Blown Film Borclear RB707CF is a propylene-ethylene copolymer film resin without slip and antiblock additives, suitable for the manufacturing of unoriented film on blown film process.Borclear RB707CF is especi.. |
|||
Melting Point | 143 °C | 289 °F | ISO 3146 |
Borealis Borclear™ RE936CF Polypropylene Random Copolymer Borclear™ RE936CF is a random copolymer. This grade is suitable for the manufacturing of unoriented films on chill roll processes. Applications: food packaging, lamination films, and stationary fil.. |
|||
Melting Point | 143 °C | 289 °F | DSC; ISO 3146 |
Borealis Bormed™ RE806CF Polypropylene Random Copolymer Bormed™ RE806CF is a random copolymer. The material is specially formulated for medical applications. Applications: Bormed™ RE806CF is recommended for medical packaging. Bormed™ RE806CF contai.. |
|||
Melting Point | 143 °C | 289 °F | |
Williams Advanced Alloys WS143 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Melting Point | 143 °C | 289 °F | DSC |
Total PPR 7238 Polypropylene, Random Copolymer - Blow Molding Impact Strength. TOTAL Polypropylene 7238 offers excellent impact strength, clarity and gloss.Lubricated 7238 offers superior core rod release for ease in processing.High Purity. 7238 features min.. |
|||
Melting Point | 143 °C | 289 °F | DSC |
Total PPR 7450HC Polypropylene, Film Extrusion Grade Random copolymer heat sealable film gradeColor - Low catalyst residuals in FINA 7450HC result in improved color stability.Clarity/Impact - The random copolymer structure of FINA 7450HC improves its .. |
|||
Melting Point | <= 143 °C | <= 289 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil EN 33330 Ethylene n-Butyl Acrylate Copolymer Resin Product Description: ExxonMobil EN 33330 is a high flow 32.5% nBA copolymer suitable for use in hot melt adhesives and sealants. Availability: Latin America, North America and South America Additive.. |
|||
Melting Point | 143 °C | 289 °F | DSC |
Arkema Group OREVAC® 18722 Maleic Anhydride Modified Polypropylene OREVAC 18722 is a maleïc anhydride modified PP based resin. It is available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyolefins. OREVAC 18722 .. |
|||
Melting Point | 143 °C | 289 °F | |
BASF Novolen® 3340 PC Polypropylene Nucleated grade for injection moldings with higher transparency.Data was collected by ISO methods and provided by BASF. |
|||
Melting Point | 143 - 165 °C | 289 - 329 °F | Average value: 148 °C Grade Count:17 |
Overview of materials for Polypropylene, Blow Molding Grade This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Blow Molding Grade". Each property range of values reported is minimum and maximum values.. |
|||
Melting Point | 143 - 151 °C | 289 - 304 °F | |
Indium Corp. Indalloy 225 Indium Solder Alloy Information Provided by Indium Corporation |