Polymer Property : Melting Point = 139 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 139 °C
282 °F
Flow temperature, ASTM D569-59
Rotuba 880 Ethyl Cellulose
Data provided by the manufacturer.
Melting Point 139 °C
282 °F
Nihon Superior BI57 Sn-Bi Lead-Free Solder Alloy
Melting Point 139 - 140 °C
282 - 284 °F
Indium Corp. Indalloy® 282 57Bi/42Sn/1Ag Lead-Free Solder Alloy
The addition of Ag adds mechanical strength. Good thermal fatigue performance; established history.Information provided by the manufacturer, Indium Corporation.
Melting Point 139 - 141 °C
282 - 286 °F
Solvay RHODAPHOSE® BIS DIPHENYL PHOSPHINO ETHANE Phosphorus Derivative
Identification: 1,2-BIS (DIPHENYLPHOSPHINO) ETHANE (DPPE).CAS: 1663 – 45 – 2Available in: Asia Pacific, Europe, Latin America and North America Applications: DPPE is a bidentate phosphine ..
Melting Point <= 139 °C
<= 282 °F
Peak Melting Point; ExxonMobil method
ExxonMobil Escorene™ UL 04331EL Ethylene Vinyl Acetate Copolymer
Product Description: UL 04331EL is a HEVA grade, especially designed for photovoltaic cells and encapsulation applications, requiring a good balance of adhesion and COF. It offers excellent light tr..
Melting Point 139 °C
282 °F
BASF Novolen® 3325 MC Polypropylene
Grade containing slip and blocking agents, for cast film.Data was collected by ISO methods and provided by BASF.
Melting Point 139 °C
282 °F
BASF Novolen® 3336 MC Polypropylene
Data was collected by ISO methods and provided by BASF.
Melting Point 139 °C
282 °F
BASF Novolen® 3300 MC Polypropylene
Data was collected by ISO methods and provided by BASF.