Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 1317 - 1367 °C | 2403 - 2493 °F | |
Special Metals INCONEL® alloy 693 INCONEL alloy 693 is a new alloy from Special Metals which offers resistance to high temperature corrosion mechanisms not previously available from a nickel-based alloy. Of particular interest to t.. |