Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 120 °C | 248 °F | Internal method |
Polimeri Europa Clearflex® H&T CLH 108 Octene Copolymer Linear Low Density Polyethylene Clearflex H&T CLH 108 is an octene copolymer linear low density polyethylene (C8-LLDPE), with antioxidants, suitable for cast film extrusion. Stretch films obtained from Clearflex H&T CLH 108 show e.. |
|||
Melting Point | 120 °C | 248 °F | Internal method |
Polimeri Europa Flexirene® FF 25 Butene Copolymer Linear Low Density Polyethylene Flexirene FF 25 is a butene copolymer linear low density polyethylene (C4-LLDPE), with antioxidants, suitable for blown film extrusion.Flexirene FF 25 is characterized by a high elongational viscosi.. |
|||
Melting Point | 120 °C | 248 °F | Internal method |
Polimeri Europa Clearflex® FG B0 Very Low Density Polyethylene Clearflex FG B0 is a linear low density polyethylene, with antioxidants, suitable for blown film technology.Films made with Clearflex FG B0 are highly transparent, have good sealing properties, even.. |
|||
Melting Point | 120 - 165 °C | 248 - 329 °F | 0.025" extruded film, |
Huntsman IROGRAN® A 70 H 4714 M TPU-Polyester Introduction: IROGRAN A 70 H 4714 M is a soft polyester based thermoplastic polyurethane intended for injection molding applications. IROGRAN A 70 H 4714 M is part of the HUNTSMAN injection molding .. |
|||
Melting Point | 120 °C | 248 °F | DIN EN ISO 314 |
GEHR Plastics ECOGEHR® PLA-LF Polylactic Acid PLA-L is a blend of polylactide, lignin, lingo-cellulosic, natural fatty acids, waxes and wood fibers. This material possesses good mechanical properties similar to ABS. This bioplastic has an opera.. |
|||
Melting Point | 120 °C | 248 °F | ASTM D3418 |
SK Chemicals SKYTHANE® SG400 SKYGREEN Biodegradable Thermoplastic SKYGREEN is a series of aliphatic polyester and aliphatic/aromatic copolyester that is degraded into water and carbon dioxide by microorganismsSKYGREEN, biodegradable thermoplastics, has been develo.. |
|||
Melting Point | 120 °C | 248 °F | DSC; ASTM D3418 |
Westlake Tymax™ GT4524 Anhydride Modified Linear Low Density Polyethylene Westlake GT4524 is an anhydride modified linear low density polyethylene designed for blown film extrusion that contains no slip and no antiblock additives. This resin is designed to function as a c.. |
|||
Melting Point | 120 °C | 248 °F | DSC |
Lubrizol ESTANE® 54610 Ester Based Thermoplastic Polyurethane Features: Good physical properties and chemical resistance and wide processing window for calendering.Uses: Melt coating/calendering, flat die/cast film extrusion.Available in Americas, Europe, Midd.. |
|||
Melting Point | 120 - 130 °C | 248 - 266 °F | DSC |
EMS-Griltech Griltex® 2A Copolyamide Hotmelt Adhesive (Apparel Interlinings) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Melting Point | 120 - 130 °C | 248 - 266 °F | DSC |
EMS-Griltech Griltex® D 1441E Copolyester Hotmelt Adhesive (Technical Applications) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Melting Point | 120 - 135 °C | 248 - 275 °F | |
DayGlo ZQ Pigments ZQ-11 Aurora Pink DAY-GLO ZQ-Pigments are an improved version of DAY-GLO Z-Pigments. They offer lower mold plateout, increased plastic compatibility, are mostly stronger, require processing temperatures, and have lar.. |
|||
Melting Point | 120 - 135 °C | 248 - 275 °F | |
DayGlo ZQ Pigments ZQ-17 Saturn Yellow DAY-GLO ZQ-Pigments are an improved version of DAY-GLO Z-Pigments. They offer lower mold plateout, increased plastic compatibility, are mostly stronger, require processing temperatures, and have lar.. |
|||
Melting Point | 120 - 180 °C | 248 - 356 °F | |
BASF Neopolen® P 9230 A 0.06 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9230 A is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9230 A.Note: In order to.. |
|||
Melting Point | 120 - 180 °C | 248 - 356 °F | |
BASF Neopolen® P 9230 D 0.06 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9230 D is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9230 D.Note: In order to.. |
|||
Melting Point | 120 - 180 °C | 248 - 356 °F | |
BASF Neopolen® P 9235 0.04 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9235 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9235.Note: In order to mea.. |
|||
Melting Point | 120 - 180 °C | 248 - 356 °F | |
BASF Neopolen® P 9255 0.09 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9255 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9255.Note: In order to mea.. |
|||
Melting Point | 120 - 180 °C | 248 - 356 °F | |
BASF Neopolen® P 9335 MG 0.04 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9333 MG is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9333 MG.Note: In order .. |
|||
Melting Point | 120 - 180 °C | 248 - 356 °F | |
BASF Neopolen® P 9335 MG 0.06 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9333 MG is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9333 MG.Note: In order .. |
|||
Melting Point | 120 - 180 °C | 248 - 356 °F | |
BASF Neopolen® P 9230 A 0.04 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9230 A is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9230 A.Note: In order to.. |
|||
Melting Point | 120 - 180 °C | 248 - 356 °F | |
BASF Neopolen® P 9230 A 0.05 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9230 A is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9230 A.Note: In order to.. |
|||
Melting Point | 120 - 180 °C | 248 - 356 °F | |
BASF Neopolen® P 9235 0.05 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9235 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9235.Note: In order to mea.. |
|||
Melting Point | 120 - 180 °C | 248 - 356 °F | |
BASF Neopolen® P 9235 0.07 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9235 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9235.Note: In order to mea.. |
|||
Melting Point | 120 - 180 °C | 248 - 356 °F | |
BASF Neopolen® P 9270 0.07 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9270 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9270.Note: In order to mea.. |
|||
Melting Point | 120 - 180 °C | 248 - 356 °F | |
BASF Neopolen® P 9270 0.11 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9270 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9270.Note: In order to mea.. |
|||
Melting Point | 120 °C | 248 °F | DSC |
Lubrizol ESTANE® 58271 Ester Based Thermoplastic Polyurethane Features: Good physical properties, chemical resistance and adhesive properties and wide processing window for extrusion.Uses: Blown and flat die/cast film extrusion, Injection and blow molding.Avai.. |