Polymer Property : Melting Point = 108 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 108 °C
226 °F
Internal method
Polimeri Europa Riblene® GP 26 Low Density Polyethylene - Coating Grade
Riblene GP 26 is a high fluidity low density polyethylene resin (LDPE).Main Applications: Riblene GP 26 is suitable for coating applications where low neck-in and high draw-down are key factors. F..
Melting Point 108 °C
226 °F
Internal method
Polimeri Europa Riblene® MQ 10 Low Density Polyethylene - Injection Molding
Riblene MQ 10 is a good fluidity low density polyethylene resin (LDPE).Parts made with Riblene MQ 10 are characterized by a high flexibility.Main Applications: Riblene MQ 10 is suitable for injecti..
Melting Point 108 °C
226 °F
Internal method
Polimeri Europa Riblene® MQ 10 R Low Density Polyethylene - Injection Molding
Riblene MQ 10 R is a good fluidity low density polyethylene resin (LDPE).Parts made with Riblene MQ 10 R are characterized by a high flexibility.Main Applications: Riblene MQ 10 R is suitable for i..
Melting Point 108 °C
226 °F
Peak Melting Temperature; ExxonMobil Method
ExxonMobil LD 146.NH Packaging Film Resin  (discontinued **)
LD 146.NH is a homopolymer film resin offering good clarity, toughness, and stiffness. It is used in food packaging and laminating film.Information provided by ExxonMobil Chemical
Melting Point 108 °C
226 °F
Exxon Method
ExxonMobil Escorene® LD-400 LDPE Medium/High Voltage Insulation  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A crosslinkable polyethylene homopolymer resin designed for electrical applications.Applications: Base resin for medium voltage power cable insulati..
Melting Point 108 °C
226 °F
LyondellBasell Lupolen® 2012 D SW 413 LDPE
Cable sheathingData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell.
Melting Point 108 °C
226 °F
LyondellBasell Lupolen® V 2520 J Ethylene Vinyl Acetate, Film Grade
FilmData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell.
Melting Point 108 - 124 °C
226 - 255 °F
ASTM D127
IRPC Polimaxx Polene PE220NSC Polypropylene Wax
APPLICATIONS: CARRIER FOR PIGMENT CONCENTRATES, LUBRICANT FOR PLASTICS, RUBBER EXTRUSION, HOT MELT ADHESIVE, PAPER COATING
Melting Point 108 - 124 °C
226 - 255 °F
ASTM D127
IRPC Polimaxx Polene PE250N Polypropylene Wax
APPLICATIONS: CARRIER FOR PIGMENT CONCENTRATES, LUBRICANT FOR PLASTICS, RUBBER EXTRUSION, HOT MELT ADHESIVE, PAPER COATING
Melting Point 108 °C
226 °F
LyondellBasell Lupolen® 2003 H LDPE, Film Grade
FilmData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell.
Melting Point 108 - 119 °C
226 - 246 °F
Indium Corp. Indalloy 61 Bismuth Solder Alloy
Information Provided by Indium Corporation
Melting Point 108 °C
226 °F
LyondellBasell Lupolen® 1800 S LDPE, Injection Molding Grade
Injection moldingsData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell.
Melting Point 108 °C
226 °F
LyondellBasell Lupolen® 1810 D LDPE
Blow moldings, sheet, profile, film.Data was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell.
Melting Point 108 °C
226 °F
LyondellBasell Lupolen® 1810 E LDPE
Blow moldingData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell.
Melting Point 108 °C
226 °F
LyondellBasell Lupolen® 1810 H LDPE, Injection Molding Grade
Injection moldingsData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell.
Melting Point 108 °C
226 °F
LyondellBasell Lupolen® 1812 E LDPE
Insulation for cableData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell.
Melting Point 108 °C
226 °F
LyondellBasell Lupolen® 1840 H LDPE
Blow moldings, injection moldings, film.Data was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell.
Melting Point 108 °C
226 °F
Upon Melting via DSC/ASTM D3418
DuPont 20 Series DPE 20 Specialty Polyethylene Resin
DuPont 20 specialty low density polyethylene resin is characterized by low melt index and intermediate crystallinity. This product, produced via a unique polymerization process, has outstanding flex..
Melting Point 108 °C
226 °F
ISO 11357
Total LDPE 1070 MN 18 C Low Density Polyethylene - Injection Molding and Compounding
LDPE 1070 MN 18 C is a low density polyethylene made by a high pressure autoclave process without antioxidant. Grade adapted to the production of flexible parts with a high production rate.Applicat..
Melting Point 108 °C
226 °F
ISO 11357
Total LDPE LA 0710 Low Density Polyethylene - Extrusion Coating
LDPE LA 0710 is a low density polyethylene made by a high pressure autoclave process without antioxidant.Application examples: coating of paper, paperboard, aluminum. High draw down, low neck in.In..
Melting Point 108 °C
226 °F
Dow Method (DSC)
Dow 621I Low Density Polyethylene (LDPE)
Specialty resin designed for high melt strength applications Provides excellent bubble stability Complies with U.S. FDA 21 CFR 177.1520 (c) 2.1 Information provided by Dow
Melting Point 108 °C
226 °F
Dow Method (DSC)
Dow 662I Low Density Polyethylene Resin
Blown Film Resin designed for enhanced bubble stability High melt strength Optimum gauge range: 1.5 - 5.0 mil Complies with U.S. FDA 21 CFR 177.1520 (c) 2.1 Information provided by Dow
Melting Point 108 °C
226 °F
ISO 11357
Carmel Olefins IPETHENE® 670 Low Density Polyethylene
IPETHENE® 670 is a low density polyethylene extrusion coating and lamination grade. This grade can be processed at high coating temperatures and coating speeds. It exhibits low neck-in and stable w..
Melting Point 108 °C
226 °F
ASTM D3418
Petroquimica Triunfo Trithene® JX 7300 LDPE - Injection Molding
The Trithene® JX 7300 resin is a low-density polyethylene (LDPE) with outstanding flow ability and flexibility. Those attributes are especially important to meet the requirements for fast injection..
Melting Point 108 °C
226 °F
ASTM D3418, ISO 3146
DuPont™ Fusabond® M603 Polymer Modifier
Fusabond® M603 Resin is a random ethylene copolymer, incorporating a monomer which is classified as being a maleic anhydride equivalent for application uses.Fusabond® M603 is used in a variety of ..