Polymer Property : Transformation Temperature = -17.2 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Transformation Temperature -17.2 °C
1.00 °F
by DSC
Lubrizol ESTANE® 58092 Ester Based Thermoplastic Polyurethane
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..