Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lubrizol ESTANE® 58092 Ester Based Thermoplastic Polyurethane

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane, TP , Thermoplastic Polyurethane, Elastomer, Polyester Grade
Manufacturer Lubrizol (former Noveon)
Trade Name ESTANE®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol ESTANE® 58092 Ester Based Thermoplastic Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability in a flexible thermoplastic elastomer system that is easy to process in a wide range of equipment. The Estane® TPU portfolio of products offers high performance polyester - and polyether - based resins and compounds in a broad range of hardnesses to meet a variety of application needs.Benefits of Estane® TPU: Outstanding Abrasion and Wear ResistanceExcellent Low Temperature FlexibilitySuperior Toughness and DurabilityEase of Processing and Manufacturing FlexibilityColorability and Paintability with no adhesion promoterApplications: Film & SheetFabric coating & melt coatingWire & CableHose, Tube & ProfileCustom moldingCustom compoundingAutomotive interior/chassis and exterior painted trimSpecific Notes for this Material: Good hydrocarbon resistance Information provided by Noveon, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.22 g/cc
1.22 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 93
93
ASTM D2240
Hardness, Shore D 45
45
ASTM D224
Tensile Strength, Ultimate 31.7 MPa
4600 psi
ASTM D412/D638
Elongation at Break 450 %
450 %
ASTM D412/D638
Flexural Modulus 0.0310 GPa
4.50 ksi
ASTM D790
Taber Abrasion, mg/1000 Cycles 2.6
2.6
CS-17; ASTM D3389 B
Compression Set 28 %
28 %
ASTM D395
Tensile Set 17 %
17 %
ASTM D412/D638
Thermal Properties Metric English Comments
Vicat Softening Point 107 °C
225 °F
ASTM D1525
Transformation Temperature -17.2 °C
1.00 °F
by DSC