Polymer Property : Ring & Ball Softening Point = 441 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Ring & Ball Softening Point 227 °C
441 °F
ASTM E28
DuPont Elvax® 770 Ethylene Vinyl Acetate
DuPont™ Elvax® 770 is a low BHT anti-oxidant ethylene-vinyl acetate copolymer resin for use in industrial applications. Applications: Elvax® 770 resins can be used for the following application..