Thermal Properties | Metric | English | Comments |
---|---|---|---|
Ring & Ball Softening Point | 82.0 °C | 180 °F | ASTM E28 |
DuPont Elvax® 210W Ethylene Vinyl Acetate DuPont™ Elvax® 210W is an ethylene-vinyl acetate copolymer resin containing an anti-blocking additive for use in industrial applications. This resin is supplied in pellet form and to prevent the p.. |
|||
Ring & Ball Softening Point | 82.0 °C | 180 °F | ASTM E28 |
Arkema Group EVATANE® 28-420 Copolymer Ethylene - Vinyl Acetate EVATANE® 28-420 is a random copolymer of Ethylene and Vinyl Acetate made by high-pressure radicalar polymerisation process. EVATANE® 28-420 is stabilized with antioxidants. The High Vinyl Acetate .. |
|||
Ring & Ball Softening Point | 82.0 °C | 180 °F | ASTM E28 |
DuPont Elvax® 210 Ethylene Vinyl Acetate
(discontinued **) DuPont™ Elvax® 210 is an ethylene-vinyl acetate copolymer resin for use in industrial applications. Applications:Elvax® 210 resins can be used for the following applications: adhesives, sealants,.. |