Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Transformation Temperature, Tg 195 °C
383 °F
DMA
SABIC Innovative Plastics ULTEM STM1600 PEI Copolymer
Siltem 1600 is a flexible copolymer designed for wire and cable applications. It offers a halogen free (according VDE 0472) flame retardant solution that also offers low smoke emission and toxicity...
Transformation Temperature, Tg 195 °C
383 °F
DMA
SABIC Innovative Plastics ULTEM STM1600 PEI Copolymer (Europe-Africa-Middle East)
Siltem 1600 is a flexible copolymer designed for wire and cable applications. It offers a halogen free (according VDE 0472) flame retardant solution that also offers low smoke emission and toxicity...