Thermal Properties | Metric | English | Comments |
---|---|---|---|
Transformation Temperature, Tg | 613 °C | 1140 °F | |
Schott KG4 Short Pass Filter Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz.Similar glasses include KG2, KG3, KG1, KG5 |
|||
Transformation Temperature, Tg | 614 °C | 1140 °F | |
Schott N-LASF43 Glass Information Provided by SCHOTT North America, Inc. |
|||
Transformation Temperature, Tg | 618 °C | 1140 °F | |
Schott N-LAK7 Glass Information Provided by SCHOTT North America, Inc. |
|||
Transformation Temperature, Tg | 616 °C | 1140 °F | |
Schott N-SSK8 Glass Information Provided by SCHOTT North America, Inc. |
|||
Transformation Temperature, Tg | 614 °C | 1140 °F | |
Schott N-LAK12 Glass Information Provided by SCHOTT North America, Inc. |