Thermal Properties | Metric | English | Comments |
---|---|---|---|
Transformation Temperature, Tg | 600 °C | 1110 °F | ISO 7884-8 |
Schott Glass 8229 Intermediate sealing glass Used for sealing to Glass 8228 and Glass 8230 The heavy metal content for the elements lead, cadmium, mercury, and hexavalent chromium is below 100 ppmInformation provided by SCHOTT AG. |
|||
Transformation Temperature, Tg | 600 °C | 1110 °F | |
Schott GG455 Long Pass Filter Colloidally colored glass. Data provided by the manufacturer, Schott Glas Mainz.Similar glasses include GG395, GG400, GG420, GG435, GG385, GG475, GG495, OG515, OG530, OG550, OG570, OG590, RG610, RG6.. |
|||
Transformation Temperature, Tg | 600 °C | 1110 °F | |
Schott GG495 Long Pass Filter Colloidally colored glass. Data provided by the manufacturer, Schott Glas Mainz.Similar glasses include GG395, GG400, GG420, GG435, GG455, GG475, GG385, OG515, OG530, OG550, OG570, OG590, RG610, RG6.. |
|||
Transformation Temperature, Tg | 600 °C | 1110 °F | |
Schott N-LAF33 Glass Information Provided by SCHOTT North America, Inc. |