Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 70.0 - 90.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
38.9 - 50.0 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-1/-2 |
Styrolution Luran® S KR 2863 C Colored ASA+PC Description: Grade with very high heat resistance for automotive interiors and exteriors as well as electrical parts.Information provided by STYROLUTION, which is a joint venture between BASF and IN.. |
|||
CTE, linear, Parallel to Flow | 70.0 - 90.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
38.9 - 50.0 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-1/-2 |
Styrolution Luran® S KR 2864 C Colored ASA+PC Description: Easy flowing injection molding grade with heat resistance for parts with thin walls and/or with adverse flowpath/wall thickness ratios.Applications: Mobile phone housings.Information pr.. |
|||
CTE, linear, Parallel to Flow | 70.0 - 90.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
38.9 - 50.0 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-1/-2 |
Styrolution Luran® S KR 2864 C UV Colored ASA+PC Description: Easy flowing injection molding grade with heat resistance for parts with thin walls and/or with adverse flowpath/wall thickness ratios.Applications: Mobile phone housings.Information pr.. |
|||
CTE, linear, Parallel to Flow | 50.0 - 90.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
27.8 - 50.0 µin/in-°F @Temperature 73.4 - 176 °F |
DIN 11359-1/-2 |
BASF Ultramid® KR 4355 G10 BK 23215 50% Glass Filled PA6/6T (Dry) Description: 50% glass-fiber reinforced product for injection molding; high toughness and rigidity; low water absorption, high melting point (285°C); mechanical properties remain constant up to 60°.. |
|||
CTE, linear, Parallel to Flow | 80.0 - 90.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
44.4 - 50.0 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-1/-2 |
BASF Ultradur® B 4300 K4 20% Glass Bead Filled PBT Description: Is a PBT + ASA, Injection-molding grades containing 20% of glass beads for industrial parts with low warpage.Applications: Precision parts for optical instruments, fuel tank sensor unit.. |
|||
CTE, linear, Parallel to Flow | 70.0 - 90.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
38.9 - 50.0 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-1/-2 |
Styrolution Luran® S KR 2861/1 C Colored ASA+PC Description: Grade with high heat resistance for injection molding and extrusion.Applications: Interior and exterior automotive parts, and electrical housings.Information provided by STYROLUTION, wh.. |
|||
CTE, linear, Parallel to Flow | 70.0 - 90.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
38.9 - 50.0 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-1/-2 |
Styrolution Luran® S KR 2863 C UV Colored ASA+PC Description: Grade with very high heat resistance for automotive interiors and exteriors as well as electrical parts.Information provided by STYROLUTION, which is a joint venture between BASF and IN.. |