Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 110 µm/m-°C @Temperature 23.0 - 60.0 °C |
61.1 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP KP004 Acetal Copolymer (Europe-Africa-Middle East) LNP* Lubricomp* KP004 is a compound based on Acetal Copolymer resin containing PTFE, Silicone. |
|||
CTE, linear, Parallel to Flow | 110 µm/m-°C @Temperature 23.0 - 80.0 °C |
61.1 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Xenoy® CL200 PBT+PC (Europe-Africa-Middle East) XENOY CL200 is a semi-crystalline thermoplastic blend, specially developed to obtain good low temperature impact strength combined with excellent chemical resistance to occasional solvent and gasoli.. |
|||
CTE, linear, Parallel to Flow | 110 µm/m-°C | 61.1 µin/in-°F | ASTM Test |
Styrolution Luran® S 797 SE ASA Luran S 797 SE is an extrusion ASA grade with especially high notched impact strength, used for sheet and profile extrusions. The data representable is based on extruded sheet.Information provided .. |
|||
CTE, linear, Parallel to Flow | 110 µm/m-°C @Temperature 20.0 °C |
61.1 µin/in-°F @Temperature 68.0 °F |
ISO 11359-2 |
Polyplastics Tepcon M130 Acetal-copolymer (POM), High Fluidity Information provided by PolyPlastics. |
|||
CTE, linear, Parallel to Flow | 110 µm/m-°C | 61.1 µin/in-°F | ISO 11359-1/-2 |
Covestro Makroblend® S 7916/2 Polycarbonate + PBT, Impact Grade ISO 7792-1-PBT/PC,MHPR,-020(PBT+PC)-blendsimpact modifiedInjection molding gradeexcellent chemical resistancehigh toughness at low temperaturesideal for painted applicationsunreinforcedPreprocessing.. |
|||
CTE, linear, Parallel to Flow | 110 µm/m-°C @Temperature 20.0 °C |
61.1 µin/in-°F @Temperature 68.0 °F |
ISO 11359-1/-2 |
DSM Arnitel® EL740 74 Shore D, Injection Grade Copolyester Elastomer (North America) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
CTE, linear, Parallel to Flow | 110 µm/m-°C @Temperature 20.0 °C |
61.1 µin/in-°F @Temperature 68.0 °F |
ISO 11359-1/-2 |
DSM Arnitel® EL740-H/A Injection Molding; Other Extrusion Grade Copolyester Elastomer (North America) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
CTE, linear, Parallel to Flow | 110 µm/m-°C @Temperature 20.0 °C |
61.1 µin/in-°F @Temperature 68.0 °F |
ISO 11359-1/-2 |
DSM Arnitel® PL581 58 Shore D, Injection Grade Copolyester Elastomer (North America) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
CTE, linear, Parallel to Flow | 110 µm/m-°C | 61.1 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® LV-23 X ESD PA12-GF23 Product description: Grilamid LV-23 X ESD black is an antistatic Polyamide 12 injection moulding grade with 23 % glass fibre reinforcement. Main attributes are: antistatic with reisitivity < 10^6 O.. |
|||
CTE, linear, Parallel to Flow | 110 µm/m-°C | 61.1 µin/in-°F | ISO 11359-1/-2 |
DuPont Performance Polymers Delrin® FG150 NC010 Acetal (POM)
(Unverified Data**) High Viscosity Acetal Homopolymer Developed for Food Contact ApplicationsDelrin FG150 NC010 is a high viscosity acetal homopolymer for extrusion processes. It has low die deposit and low porosity. I.. |
|||
CTE, linear, Parallel to Flow | 110 µm/m-°C @Temperature 23.0 - 55.0 °C |
61.1 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1/-2 |
BASF Ultraform® S2320 003 POM Description: Easy flowing and rapidly freezing grade for injection molding difficult, thin-walled part.Information provided by BASF |