Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 8.30 µm/m-°C @Temperature 40.0 - 120 °C |
4.61 µin/in-°F @Temperature 104 - 248 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP KONDUIT OX11315 PPS (Asia Pacific) Thermally conductive electrically insulative mineral filled PPS FR compound. |