Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 46.8 µm/m-°C | 26.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PEEK 150 Availability: North AmericaForms: PelletsFeatures: Low ViscosityInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 46.8 µm/m-°C | 26.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PEEK 450 BK Availability: North AmericaForms: PelletsFeatures: High ViscosityAppearance: BlackInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 46.8 µm/m-°C | 26.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PEEK HF Availability: North AmericaForms: PelletsFeatures: Low ViscosityInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 46.8 µm/m-°C | 26.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® POM CO GF10 CC 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforced, 10% Filler by WeightFeatures: Copolymer and Chemically CoupledInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 46.8 µm/m-°C | 26.0 µin/in-°F | ASTM D696 |
Techmer ES Luriblend® HTN 01420 BK Availability: North AmericaForms: PelletsAdditive: Molybdenum Disulfide LubricantFeatures: Good Wear Resistance, Low Friction, High Heat Resistance and LubricatedAppearance: BlackInformation provide.. |
|||
CTE, linear, Parallel to Flow | 46.8 µm/m-°C | 26.0 µin/in-°F | ASTM D696 |
Techmer ES Luriblend® PA6 ML2 HS BK Nylon 6 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and Molybdenum Disulfide Lubricant(2%)Features: Good Wear Resistance, Low Friction, Heat Stabilized and LubricatedAppearance: Blac.. |
|||
CTE, linear, Parallel to Flow | 46.8 µm/m-°C | 26.0 µin/in-°F | ASTM D696 |
Techmer ES Luriblend® PA6 ML2 Nylon 6 Availability: North AmericaForms: PelletsAdditive: Molybdenum Disulfide Lubricant(2%)Features: Good Wear Resistance, Low Friction and LubricatedInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 46.8 µm/m-°C | 26.0 µin/in-°F | ASTM D696 |
Techmer ES Luriblend® PA6 ML3 BK Nylon 6 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and Molybdenum Disulfide Lubricant(3%)Features: Good Wear Resistance, Low Friction, Heat Stabilized and LubricatedAppearance: Black.. |
|||
CTE, linear, Parallel to Flow | 46.8 µm/m-°C | 26.0 µin/in-°F | ASTM D696 |
Techmer ES Luriblend® PA6/6 ML2 Nylon 66 Availability: North AmericaForms: PelletsAdditive: Molybdenum Disulfide Lubricant(2%)Features: Lubricated and Good Wear ResistanceInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 46.8 µm/m-°C | 26.0 µin/in-°F | ASTM D696 |
Techmer ES Luriblend® POM CO CF10 TL10 BK 10% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 10% Filler by WeightAdditive: PTFE Lubricant(10%)Features: Lubricated and CopolymerUL File: E157318Information provided b.. |
|||
CTE, linear, Parallel to Flow | 46.8 µm/m-°C | 26.0 µin/in-°F | ASTM D696 |
Techmer ES Luriblend® HTN 01410 BK Availability: North AmericaForms: PelletsAdditive: Graphite Powder Lubricant and Molybdenum Disulfide LubricantFeatures: Good Wear Resistance, Low Friction, High Heat Resistance and LubricatedAppear.. |