Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 30.5 µm/m-°C @Temperature 20.0 °C |
16.9 µin/in-°F @Temperature 68.0 °F |
ASTM data |
Dow Questra® EA503 High Heat Syndiotactic Polystyrene, 30% Glass Filled
(discontinued **) QUESTRA® Crystalline Polymers are semi-crystalline engineering thermoplastic resins produced from styrene monomer using a proprietary metallocene catalyst system. These syndiotactic polymers are ve.. |
|||
CTE, linear, Parallel to Flow | 30.5 µm/m-°C @Temperature 20.0 °C |
16.9 µin/in-°F @Temperature 68.0 °F |
ASTM data |
Dow Questra® EA513 High Heat Syndiotactic Polystyrene, 30% Glass Filled
(discontinued **) QUESTRA® Crystalline Polymers are semi-crystalline engineering thermoplastic resins produced from styrene monomer using a proprietary metallocene catalyst system. These syndiotactic polymers are ve.. |